| MICROSTRUCTURE TRANSITION OF SUPERCOOLED DZ125 SUPERALLOY |
| ZHOU Jun1; XIE Faqin1; WU Xiangqing1; ZHANG Jun2 |
1.School of Aeronautics; Northwestern Polytechnical University; Xi'an 710072
2.State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
ZHOU Jun XIE Faqin WU Xiangqing ZHANG Jun . MICROSTRUCTURE TRANSITION OF SUPERCOOLED DZ125 SUPERALLOY. Acta Metall Sin, 2009, 45(4): 385-389.
|
|
|
Abstract Investigations of microstructural evolution in undercooled metallic melts have been extensively conducted in different alloy systems, such as eutectic, peritectic and metallic compound, however, few reports about undercooled superalloys were found up to date. In this paper, DZ125 superalloy melt was undercooled by the method of molten salt purification combined with cycled superheating under Ar atmosphere, and a substantial undercooling up to 180 K was obtained. Based on the microstructural observation as well as the calculations of the dendritic tip radius, the dendrite growth velocity and undercooling with BCT (Boettinger, Coriell, Trivedi) dendrite growth model, the solidification behavior and structure transition mechanisms were systematically investigated. The results indicate that the microstructure undergoes three sequent transitions in the achieved range of undercooling range ΔT. When ΔT<48 K, the dendrite growth is mainly controlled by solute diffusion, and the solidification structures are the common dendrites. When 48 K≤ΔT< 85 K, the dendrites is remelted and the first kind of granular grains forms because of the serious remelting produced by recalescence. When 85≤ΔT<160 K, the effect of solute diffusion is weakened by solute trapping that results from high dendrite growth velocity, thermal diffusion plays the dominate role at the same time, the remelting effect decreases to a low level, and ripenings of dendrite are restrained, the granular grains turn into highly developed fine dendrites. WhenΔT>160 K, the second kind of granular grains is formed, the transition is caused by the stress originating from the rapid solidification contraction, which results in the recrystallization of the fine dendrite.
|
|
Received: 01 August 2008
|
|
|
| [1] Xie F Q, Li J S, Fu H Z. Chin Sci Bull, 1999; 44: 1947
(谢发勤, 李金山, 傅恒志. 科学通报, 1999; 44: 1947)
[2] Li J F, Liu Y C, Yang G C, Zhou Y H. J Cryst Growth, 1998; 192: 462
[3] Loser W, Lindenkreuz H G, Hermann R , Shuleshova O, Woodcock T G. Mater Sci Eng, 2005; A413–414: 398
[4] Lee K L, Kui H W. Acta Mater, 2000; 48: 2117
[5] Perepezko J H, Hildal K. Mater Sci Eng, 2008; B48: 171
[6] Chen L F, Chen X S. Acta Phys Sin, 1996; 45: 169
(陈立凡, 陈熙琛. 物理学报,1996; 45: 169)
[7] Willnecker R , Herlach D M, Feuerbacher B. Phys Rev Lett, 1989; 62: 2707
[8] Chen Y Z, Liu F, Yang G C, Liu N, YanC L, Xie H, Zhou Y H. Mater Charact, 2008; 59: 412
[9] Liu N, Yang G C, Liu F, Chen Y Z, Yang C L, Zhou Y H. Acta Metall Sin, 2007; 43: 449
(刘 宁, 杨根仓, 刘 峰, 陈豫增, 杨长林, 周尧和. 金属学报,2007; 43: 449)
[10] Liu N, Liu F, Yang G C, Chen Y Z, Yang C L, Li J S, Zhou Y H. J Alloys Compd, 2008; 455: 6
[11] Galenkoa P K, Reutzela S, Herlacha D M. Acta Mater, 2007; 55: 6834
[12] Liu L Q, Zhang Z M, Xu C J, Guo X F. Acta Metall Sin, 2007; 43: 1138
(刘丽琴, 张忠明, 徐春杰, 郭学锋. 金属学报, 2007; 43: 1138)
[13] Zang D Y, Wang H P, Wei B B. Acta Phys Sin, 2007; 56: 4804
(臧渡洋, 王海鹏, 魏炳波. 物理学报, 2007; 56: 4804)
[14] Lux B, Haour G, Mollard F. Acta Metall, 1981; 35: 1235
[15] Stanescu J, Sahm P R. Ing Werkst, 1990; 2: 64
[16] Ludwiga A, Wagnera I, Laakmannb J, Sahma P R. Mater Sci Eng, 1994; A178: 299
[17] Liu F, Cai Y, Guo X F, Yang G C. Mater Sci Eng, 2000; A291: 9
[18] Liu F, PhD Thesis, Northwestern Polytechnical Univer-sity, Xi’an, 2001
(刘峰. 西北工业大学博士学位论文, 西安, 2001)
[19] Boettinger W J, Coriell S R, Trivedi R. In: Mehrabian R, Parrish P A, eds., Rapid Solidification Processing: Prin-ciples and Technologies. Vol. IV, Claitors Publishing Division, Baton Rouge, LA, 1988: 13
[20] Guo Y G, Li S M, Liu L, Fu H Z. Acta Metall Sin, 2008; 44: 365
(郭勇冠, 李双明, 刘 林, 傅恒志. 金属学报, 2008; 44: 365)
[21] Aziz M J. J Appl Phys, 1982, 53: 1158
[22] Barth M, Wei B, Herlach D M, Feuerbacher B. Mater Sci Eng, 1994; A178: 305
[23] Jackson K A, Hunt J D, Uhlmnn D R, Seward T P. Trans Met Soc AIME, 1966, 234: 149
[24] Guo X F. PhD Thesis, Northwestern Polytechnical Uni-versity, Xi’an, 1999
(郭学锋. 西北工业大学博士学位论文, 西安, 1999) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|