Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (4): 385-390     DOI:
Research Articles Current Issue | Archive | Adv Search |
Research on the ternary compound T1 with low Nd content in the Mg-Zn-Nd alloys
;
东北大学
Cite this article: 

;. Research on the ternary compound T1 with low Nd content in the Mg-Zn-Nd alloys. Acta Metall Sin, 2008, 44(4): 385-390 .

Download:  PDF(731KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The structure, composition range and phase equilibrium of the ternary compound T1 with low Nd content in the Mg-Zn-Nd alloys have been investigated by scanning electron microscopy, electron probe microanalysis, X-ray diffraction and electron diffraction. It has been shown that the ternary compound T1 with the hcp structure, whose structure parameters are a=b=1.5nm, c=0.87nm, exists in the Mg-Zn-Nd alloys with low Nd content. The composition range of the T1 phase is 27.0~33.4at%Mg, 60.0~66.4at%Zn and 6.1~7.4at%Nd. At the temperature range of 300~400℃, there exists (Mg)+T1 two-phase field; and the Zn content in the (Mg) which is in two- phase equilibrium with T1 increases with the temperature. Three-phase field T1+(Mg)+MgZn exists at 300℃, T1+MgZn+L exists at 350℃, and T1+Mg2Zn3+L exists at 400℃ in the Mg-Zn-Nd system.
Key words:  Mg-Zn-Nd system      ternary compound      structure and composition      phase equilibrium      
Received:  10 October 2007     
ZTFLH:  TG111  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I4/385

[1]Wu A R,Xia C Q.Mater Des,2007;28:1963
[2]Nie J F,Muddle B C.Acta Mater,2000;48:1691
[3]Honma T,Ohkubo T,Hono K,Kamado S.Mater Sci Eng, 2005;A395:301
[4]Honma T,Ohkubo T,Kamado S,Hono K.Acta Mater, 2007;55:4137
[5]Meng F G,Wang J,Liu H S,Liu L B,,Jin Z P.Mater Sci Eng,2007;A454-455:266
[6]Appsa P J,Karimzadehb H,Kingb J F,Lorimer G W. Scr Mater,2003;48:1023
[7]Gao X,Nie J F.Scr Mater,2007;56:645
[8]Gao X,Nie J F.Scr Mater,2007;57:655
[9]Wei L Y,Dunlop G L,Westengen H.Metall Mater Trans, 1995;26:1947
[10]Jain C C,Bai C Y,Chen S W,Koo C H.Mater Trans, 2007;48:1149
[11]Li Q,Wang Q D,Wang Y X,Zeng X Q,Ding W J.J Alloys Compd,2007;427:115
[12]Villars P,Prince A,Okamoto H.Handbook,of Ternary Al- loy Phase Diagrams,CD-ROM,Metals Park,Ohio:ASM International,1997
[13]Sugiyama K,Yasuda K,Ohsuna T,Hiraga K.Z Kristal- lographie,1998;213:537
[14]Eckhard U,Stefan B,Wolf A,Gruner D,Kreiner G.J Cryst Growth,2005;275:1987
[15]Dobatkina T V,Muratova E V,Drozdova I I.Russ Metall (Engl Trans),1987;(1):205
[16]Drits M E,Drozdova E I,Korol'kova I G,Kinzhibalo V V,Tyvanchuk A T.Russ Metall(Engl Trans),1989;(2): 195
[17]Padezhnova E M,Mel'nik E V,Dobatkina T V.Izv Akad Nauk SSSR,Met,1979;(1):217
[1] LI Hongxiao REN Yuping MA Qianqian JIANG Min QIN Gaowu. PHASE EQUILIBRIUM IN THE LOW-Ca SIDE OF Mg-Zn-Ca SYSTEM AT 400 ℃[J]. 金属学报, 2012, 48(1): 70-75.
[2] LI Hongxiao MA Qianqian REN Yuping JIANG Min QIN Gaowu. TERNARY COMPOUNDS AND RELATIVE PHASE EQUILIBRIA IN THE Mg-RICH SIDE OF THE Mg-Zn-Ca SYSTEM[J]. 金属学报, 2011, 47(4): 385-390.
[3] XIE Yu ZHANG Yan CHEN Rongshi HAN Enhou. RELATIONSHIP OF COMPOSITIONS, PHASE CONSTITUENTS AND SOLIDIFICATION PATHS OF CASTING Mg-Al-Zn ALLOYS[J]. 金属学报, 2009, 45(11): 1396-1401.
[4] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[5] LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM[J]. 金属学报, 1998, 34(9): 897-902.
[6] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[7] LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM[J]. 金属学报, 1996, 32(11): 1171-1176.
[8] QIN Gaowu;HAO Shiming;ZENG Ninghua (Northeastern University;Shenyang 110006)(Manuscript received 1994-11-04;in revised form 1995-05-04). α(α_2)/γ PHASE EQUILIBRIA IN Ti-Al-Ga AND Ti-Al-Nb-Cr SYSTEMS[J]. 金属学报, 1995, 31(23): 484-488.
[9] LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM[J]. 金属学报, 1992, 28(7): 50-54.
[10] HAO Shiming; JIANG Min (Northeast University of Technology; Shenyang). TWO-PHASE EQUILIBRIUM CALCULATION BY THE GRAND POTENTIAL METHOD FOR BINARY ALLOYS[J]. 金属学报, 1992, 28(11): 54-58.
No Suggested Reading articles found!