STUDY OF THE SCALING LAW FOR VISCOSITY COEFFICIENTS IN SIMPLE MELTS
广西大学物理科学与工程技术学院
Cite this article: 

. STUDY OF THE SCALING LAW FOR VISCOSITY COEFFICIENTS IN SIMPLE MELTS. Acta Metall Sin, 2006, 42(12): 1262-1266 .

Download:  PDF(757KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Employing a realistic many-body potentials for a series of simple melts, including Ag, Al, Au, Co, Cu, Mg, Ni, Pb, Pd, Pt, Rh, and Si, we examined by the molecular-dynamics simulation the scaling laws of viscosity with different expression of the reduction parameters. Our simulation results give the sound support to early attempts at finding the universal scaling laws proposed by Rosenfeld for transport coefficients in liquid metals. Following Dzugutov, we have also arrived at a universal scaling relationship between the viscosity coefficient and excess entropy. In particular, we find that there exists a link between the scaling law and the Arrhenius law, i.e., the excess entropy scaling law for the viscosity coefficient can be interpreted as a straightforward extension of the Arrhenius law.
Key words:  Scaling law      viscosity coefficient      excess entropy      
Received:  31 March 2006     
ZTFLH:  TG146.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I12/1262

[1] Iida T, Guthrie R I. The Physical Properties of Liquid Metal. Oxford: Clarendon, 1993: 148
[2] Rosenfeld Y. Phys Rev, 1977; 15A: 2545
[3] Rosenfeld Y. J Phys: Condens Matter, 1999; 11: 5415
[4] Arai T, Shirasuna T. J Non-Cryst Solids, 2002; 312-314: 208
[5] Grover R, Hoover W G, Moran B. J Chem Phys, 1985; 83: 1255
[6] Yokoyama I, Tsuchiya S. J Non-Cryst Solids, 2002; 312- 314: 232
[7] Dzugutov M. Nature, 1996; 381: 137
[8] Baranyai A, Evans D J. Phys Rev, 1989; 40A: 3817
[9] Bretonnet J L. J Chem Phys, 2004; 120: 11100
[10] Cleri F, Rosato V. Phys Rev, 1993; 48B: 22
[11] Ercolessi F, Adams J B. Eur Phys Lett, 1994; 26: 583
[12] Stillinger F H, Weber T A. Phys Rev, 1985; 31B: 5262
[13] Tersoff J. Phys Rev, 1988; 38B: 9902
[14] Tersoff J. Phys Rev, 1989; 39B: 5566
[15] Andersen H C. J Chem Phys, 1982; 72: 2383
[16] Hoyt J J, Asia M, Sadigh B. Phys Rev Lett, 2000; 85: 594
[1] LIU Junming;LIU Zhiguo;WU Zhuangchun Nanjing University Lecturer;National Laboratory of Solid State Microstructures;Nanjing University; Nanjing 210008. SCALING LAW OF IRREGULAR EUTECTIC IN DIRECTIONAL SOLIDIFICATION[J]. 金属学报, 1993, 29(3): 11-18.
No Suggested Reading articles found!