Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (12): 1259-1261     DOI:
Research Articles Current Issue | Archive | Adv Search |
FRACTAL ANALYSIS OF TEMPERATURE-INDUCED DISCONTINUOUS LIQUID STRUCTURAL CHANGE
合肥工业大学材料学院
Cite this article: 

. FRACTAL ANALYSIS OF TEMPERATURE-INDUCED DISCONTINUOUS LIQUID STRUCTURAL CHANGE. Acta Metall Sin, 2006, 42(12): 1259-1261 .

Download:  PDF(512KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  As a new and important problem in condensed state physics, the discontinuous structural change of liquid with temperature rising is testified by various experimental technologies. However, fractal language has been more and more frequently used to describe some disordered physical systems except liquid alloys. This paper has successfully implemented fractal ideas to observe fractal structures in liquid In-Sn alloy and considers its fractal dimension as a physical quantity sensitive to structure. Moreover, from the fractal viewpoint, the mutation of the fractal dimension has indicated once again that the liquid structure change discontinuously with temperature rising.
Key words:  liquid alloys structure      fractal theory      temperature-induced      
Received:  04 April 2006     
ZTFLH:  O552.41  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I12/1259

[1] Gefen Y, Mandelbrot B B. Phys Rev Lett, 1980; 45: 855
[2] Zu F Q, Zhu Z G, Guo L J, Zhang B, Shui J P, Liu C S. Phys Rev, 2001; 64B: 180203
[3] Zu F Q, Zhu Z G, Guo L J, Qin X B, Yang H, Shan W J. Phys Rev Lett, 2002; 89: 125505
[4] Li X F, Zu F Q, Ding H F, Yu J, Liu L J, Li Q, Xi Y. Physica, 2005; 358B: 126
[5] Wang L, Bian X F, Liu J T. Phys Lett, 2004; 326A: 429
[6] Waseda Y. The Structure of Non-Crystalline Materials. New York: McGraw-Hill, 1980: 1
[7] Chu W Y, Su Y J, Gao K W, He J Y, Li J X, Qiao L J. Fractals in Materials Science. Beijing: Chemical Industry Press, 2004: 63 (楮武扬,宿彦京,高克玮,何健英,李金许,乔利杰.材料科学中的分形.北京;化学工业出版社,2004:63)
[8] Yang Z R. Fractal Physics. Shanghai: Shanghai Scientific and Technological Education Publishing House, 1996: 4 (杨展如.分形物理学.上海:上海科技教育出版社, 1996:4)
[9] Elliott S R. Nature, 1991; 354: 445
[10] Deng Z J. Ultrafine Particle and Fractal. Chongqing: Southwest China Normal University Press, 1993: 1 (邓昭镜.超微粒与分形.重庆:西南师范大学出版社, 1993: 1)
[11] Bian X F, Liu X F, Ma J J. Heredity in Cast Metals. Jinan: Shandong Science & Technology Press, 1998: 1 (边秀房,刘相法,马家骥.铸造金属遗传学.济南:山东科学技术出版社,1998:1)
No related articles found!