Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (10): 1087-1090     DOI:
Research Articles Current Issue | Archive | Adv Search |
STUDY ON MECHANISM OF ENTRAPMENT IN SLAB CONTINUOUS CASTING MOULD WITH HIGH CASTING SPEED AND ARGON BLOWING
东北大学材料与冶金学院
Cite this article: 

. STUDY ON MECHANISM OF ENTRAPMENT IN SLAB CONTINUOUS CASTING MOULD WITH HIGH CASTING SPEED AND ARGON BLOWING. Acta Metall Sin, 2006, 42(10): 1087-1090 .

Download:  PDF(210KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  ABSTRACT A physical model was established to study the mechanism of molten slag behavior in slab continuous casting mould with high casting speed and argon blowing, and the effects of operation parameters on the liquid surface level oscillation and the slag entrapment were investigated. The results showed that slag entrapment was mainly caused by the turbulent large bubbles at the interface of slag and molten steel in mould with high casting speed and gas bubbling, and the vortex at the surface also was the way to cause slag entrapment, but there is no phenomenon of entrapment occurring due to high shear stress that was mentioned the main reason previously. In addition, the behavior and mechanism of typical slag entrapment were discussed, and the measures to eliminate slag entrapment were also presented.
Key words:  continuous casting mould      high casting speed      argon blowing      mechanism of entrapment      physical modeling      
Received:  07 March 2006     
ZTFLH:  TF777.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I10/1087

[1]Gupta D,Lahiri A K.Metall Mater Trans,1996;27B:695
[2]Iguchi M,Tomoyuki J,Mizuno Y.ISIJ Int,2000;40:685
[3]Tanaka H,Kuwatori H,Nishihara R.Tetsu Hagané,1992;78:761(田中宏幸,锹取英宏,西原良治.铁ヒ钢,1992;78:761)
[4]Theodorakakos A,Bergeles G.Metall Mater Trans,1998;29B:1321
[5]Wang Z,Mukai K,Izu D.ISIJ Int,1999;39:154
[6]McDavid R M,Thomas B G.Metall Mater Trans,1996;27B:672
[7]Panaras G A,Theodorakakos A,Bergeles G.Metall Mater Trans,1998;29B:1117
[8]Lei H,Xu H H,Zhu M Y,Gan Y,Liu X,Ni M S,Liu J Q.Iron Steel,1999;34(8):20(雷洪,许海虹,朱苗勇,干勇,刘新,倪满森,刘家奇.钢铁,1999;34(8):20)
[9]Wen G H,Li G,Zhang J C.Iron Steel,1997;32(Suppl.):691(文光华,李刚,张建春.钢铁,1997;32(suppl.):691)
[10]BaoY P,Zhu J Q,Jiang W,Wang C X,Tian N Y,Xu B M.J Univ Sci Technol Beijing,2000;22:409(包燕平,朱建强,蒋伟,王昌旭,田乃嫒,徐宝美.北京科技大学学报,2000;22:409)
[11]Tan L J,Shen H F,Liu B C,Liu X,Xu R J,Li Y Q.Acta Metall Sin,2003;39:4(谭利坚,沈厚发,柳百成,刘晓,徐荣军,李永全.金属学报,2003;39:4)
[12]Qian Z D,Wu Y L.Acta Metall Sin,2004;40:1(钱忠东,吴玉林.金属学报,2004;40:1)
[13]Hu H,Zhao H M,Zhang J M,Wang X H,Wang W J.Iron Steel Vanadium Titanium,2005;26(1):1(胡皓,赵和明,张炯明,王新华,王万军.钢铁钒钛,2005;26(1):1)
[1] YU Zhan ZHANG Zhenqiang REN Zhongming LEI Zuosheng DENG Kang. STUDY ON THE FLUID FLOW IN SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE[J]. 金属学报, 2010, 46(10): 1275-1280.
[2] MENG Xiangning ZHU Miaoyong. ANALYSIS OF LIQUID FLUX CONSUMPTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2009, 45(4): 485-489.
[3] YU Hai-Qi. MULTIPHASE FLOW PHENOMENA IN A SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE AND ARGON GAS INJECTION[J]. 金属学报, 2008, 44(5): 619-625 .
[4] Xiang-Ning MENG; Miao-Yong ZHU. ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. 金属学报, 2008, 44(10): 1193-1197 .
[5] Xiang-Ning MENG; Xu-Dong LIU. STUDY ON NON-SINUSOIDAL OSCILLATION FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED Ⅰ. Mechanism of Oscillation Marks Formation[J]. 金属学报, 2007, 43(8): 839-846 .
[6] GUO Liangliang; YAO Man; YIN Hebi; WANG Xudong; FANG Dacheng; LIU Xiao; YU Yan. CALCULATION AND DISCUSSION ON THE HEAT FLUX IN MOULD OF CONTINUOUS CASTING ROUND BILLET[J]. 金属学报, 2006, 42(9): 983-988 .
[7] YIN Hebi; YAO Man. Inverse Algorithm of Heat Transfer in Round Billet Continuous Casting Mould[J]. 金属学报, 2005, 41(6): 638-644 .
[8] ZHU Miaoyong; (Department of Ferrous Metallurgy; Northeastern University;Shenyang 110006) INOMOTO Takeo; XIAO Zeqiang(Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Futtsu; Japan). MATHEMATICAL AND PHYSICAL MODELING OF FLOW AND MIXING IN LADLES STIRRED BY ARGON THROUGH MULTI-TUYERE[J]. 金属学报, 1995, 31(22): 435-439.
No Suggested Reading articles found!