Abstract The structure, thermodynamic, hydrogen storage capacity, plateau pressure
of LaNi5-xMx(M=Al, Mn) hydrides have been investigated.
A relationship among x, the plateau pressure and the temperature is
derived from the experimental data. The influences of the lattice parameter
and cell volume, the stability of alloys on the hydrogen storage properties
are discussed. As a result, LaNi5-xMnx alloys with larger cell
volumes compared with LaNi5-xAlx alloys have lower plateau
pressure. The anisotropic degree of the crystal volumes expansion in
directions of the a and c axis and the change of stability of
LaNi5-xMx alloys as a function of the Mn content are smaller
than that as a function of the Al content. It is in agreement with the
unconspicuous attenuation of hydrogen storage capacity in
LaNi5-xMnx.
|
|
Received: 17 June 2004
|
|
|
[1]Kuijpers F A, Loopstra B O. J Phys Chem Sol, 1974; 35: 301 [2]Nakamura H, Nguyen-Manh D, Pettifor D G. J Alloys Compd, 1998; 281: 81 [3]Kisi E H, Wu E, Kemali M. J Alloys Compd, 2002; 330- 332: 202 [4]Wang X L, Suda S. Z Phys Chem, 1989; 164: 1235 [5]Dayan D, Mintz M H. J Less-Common Met, 1980; 73: 15 [6]Paul-Boncour V, Joubert J M, Latroche M, Percheron- Guegan A. J Alloys Compd, 2002; 330-332: 246 [7]Mendelsohn M H, Gruen D M, Dwight A E. Nature, 1977; 269: 45 [8]Takeshita T, Malik S K, Wallace W E. J Solid State Chem, 1978; 23: 271 [9]Mendelsohn M H, Gruen D M, Dwight A E. J Leas-Common Met, 1979; 63: 193 [10]Lartigue C, Percheron-Guegan A, Achard J G, Tasset F. J Less-Common Met, 1980; 75: 23 [11]Ide T, Sakai F, Yorozu M. Fusion Technol, 1988; 14: 769 [12]Xiao J M, Zhu F W. The Subject of Materials Energy. Shanghai: Shanghai Science & Technology Press, 1999: 256 (肖纪美,朱逢吾.材料能量学.上海:上海科技出版社,1999: 256) [13]Zhao S, Lin Q, Chen N, Ma L, Ye W. Ada Metall Sir, 1999;35:65 (赵爽,林勤,陈宁,马丽,叶文.金属学报,1999; 35:65) [14]Szajek A, Jurczyk M, Rajewski W. J Alloys Compd, 2000; 307: 290 [15]Westlake D G. J Less-Common Met, 1983; 91: 1 [16]Zhang R J, Lu M Q, Cao D L, Chen D M, Yang K. Rare Met, 2004; 28: 678 (张瑞静,吕曼祺,曹大力,陈德敏,杨柯.稀有金属,2004; 28:678) [17]Lartigue C, Percheron-Guegan A, Achard J G. J Less-Common Met, 1980; 75: 23 [18]Walters R T. J Less-Common Met, 1990; 157: 97 [19]Percheron-Guegan A, Latigue C, Achard J C, Germi P, Tasset F. J Less-Common Met, 1980; 74: 1 [20]Luder C E, Lynch F E, Magee C B. J Less-Common Met, 1977; 56: 19 [21]Switendick A C. Z Phys Chem, 1979; 117: 89 [22]Westlake D G. J Less-Common Met, 1980; 75: 177 [23]Westlake D G. J Less-Common Met, 1983; 90: 251 [24]Westlake D G. J Less-Common Met, 1983; 91: 275 [25]Lartigue C, Percheron-Guegan A, Achard J C. J Less Common Met, 1984; 101: 391 [26]Miedema A R. J Less-Common Met, 1975; 41: 283; 1976; 46: 67 [27]Gruen D M, Mendelsohn M. J Less-Common Met, 1977; 55: 149 [28]Percheron-Guegan A, Lartigue C, Achard J G. J Less-Common Met, 1985; 109: 287 [29]Gupta M. J Alloys Compd, 1999; 293-295: 190 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|