Toughness Of Heat--Affected Zone Of 800 MPa Grade Low Alloy Steel
ZHAO Lin; ZHANG Xudong; CHEN Wuzhu
Department of Mechanical Engineering; Tsinghua University; Beijing 100084
Cite this article: 

ZHAO Lin; ZHANG Xudong; CHEN Wuzhu. Toughness Of Heat--Affected Zone Of 800 MPa Grade Low Alloy Steel. Acta Metall Sin, 2005, 41(4): 392-396 .

Download:  PDF(269KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and toughness of the coarse--grained heat--affected zone (CGHAZ) in laser welding of RPC (relaxation--precipitation controlling transformation) steel were investigated by thermal simulation with a Gleeble-1500 thermal simulator. The influence of the time cooled from 800-500℃, t8/5(0.3-30 s), on the microstructure of CGHAZ and the low temperature toughness were discussed. The experimental results indicate that the granular bainite is the dominate microstructure of the CGHAZ in laser welding of RPC steel, and the impact energy of the CGHAZ is much higher than that of base metal when t8/5 is between 3 s and 8 s. Considering the effect of the size, volume, number and shape of the M-A constituent on the toughness, a toughness factor of the M-A constituent is defined. As the toughness factor increases, the toughness of the granular bainite increases. The varied trend of the impact toughness with t8/5 is mainly determined by the toughness factor of the M-A constituent.
Key words:  ultra-fine low alloy steel      coarse-grained heat-affected zone      
Received:  13 July 2004     
ZTFLH:  TG142.2  
  TG401  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I4/392

[1]Wang X M, He X L, Yang S W, Shang C J, Wu H B. ISIJ Int, 2002; 42: 1553
[2]Wang X M, Shang C J, Yang S W, He X L. Acta Metall Sin, 2002; 38: 661 (王学敏,尚成嘉,杨善武,贺信莱.金属学报,2002;38:661)
[3]Ma C Y, Tian Z L, Du Z Y, Peng Y, Zhang Z Y. Trans Chin Weld Inst, 2004; 25(2): 23 (马成勇,田志凌,杜则裕,彭云,张志勇.焊接学报,2004; 25(2):23)
[4]Peng Y, Wang G, Chen W Z. Trans Chin Weld Inst, 2001; 22: 31 (彭云,王成,陈武柱.焊接学报, 2001;22(1):31)
[5]Zhang X D, Chen W Z, Wang C. Appl Laser, 2000; 20: 104 (张旭东,陈武柱,王成.应用激光, 2000;20:104)
[6]Matsuda F, Ikeuchi K, Okada H, Hrivnak I, Park H S. Trans JWRI, 1994; 23: 231
[7]Zheng S L, Tu M J, Yan W B, Zhang P S. Acta Metall Sin, 1988; 24: SA172 (郑森林,涂铭旌,鄢文彬,张平生.金属学报,1988;24:SA172)
[8]Chen J H, Kikuta Y, Araki T, Yoneda M, Matsuda Y. Acta Metall, 1984; 32: 1779
[9]Fang H S, Deng H J. Mater Mech Eng, 1981; 5(1): 5 (方鸿生,邓海金.机械工程材料, 1981;5(1):5)
[10]Nakanishi M, Komizo Y, Fukada Y. Quarterly J. Jpn Weld Soc, 1986; 4: 447
[11]Uchino K, Ohno Y. Tetsu-to-Hagane, 1986; 72: sl159 (内野耕一,大野恭秀.铁 钢, 1986;72:s1159)
[12]Tian D W, Karjalainen L P, Qian B N, Chen X F. JSME Int J, 1997; 40A: 179
[13]Lam K Y, Wen C, Tao Z. Engng Frac Mech, 1993; 44: 753
[14]Yin G Q, Gao J S, Hong Y C, Chen R. Trans Chin Weld Inst, 2001; 22(2): 71 (尹桂全,高甲生,洪永昌,陈锐.焊接学报, 2001;22(2): 71)
[15]Kawabata F, Itakura N, Jing H Y, Amano K, Minami F, Toyoda M. JSNAJ, 1993; 173: 349
[16]Qian B N, Li J L, Si C Y, Yi Y Y. Chin J Mater Res, 1995; 9: 119 (钱百年,李晶丽,斯重遥,易耀勇.材料研究学报, 1995;9: 119)
[1] GUO Xuming; YANG Chenggang; QIAN Bainian; XU Qiang; ZHANG Hongyan. Effects Of Inoculants Ti And Zr On The Microstructures And Properties Of 2219 Al--Cu Alloy Welds[J]. 金属学报, 2005, 41(4): 397-400 .
No Suggested Reading articles found!