Deformation~ Features Of AZ31 Mg--Alloy In Initial Period Of High Temperature Creep
LI Yingjie; LIU Shimin; WU Shiding; ZHANG Zhefeng; WANG Zhongguang
Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
Cite this article: 

LI Yingjie; LIU Shimin; WU Shiding; ZHANG Zhefeng; WANG Zhongguang. Deformation~ Features Of AZ31 Mg--Alloy In Initial Period Of High Temperature Creep. Acta Metall Sin, 2005, 41(4): 380-384 .

Download:  PDF(420KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue life, surface deformation morphology, fatigue cracking and fatigue fractography of Al-0.7%Cu (mass fraction) alloy, produced by equal channel angular pressing (ECAP) for 4 passes, were investigated under constant stress or plastic strain control. It is shown that the specimens displayed obvious cyclic softening, which caused some difference in fatigue life at low or high stress range under constant stress and strain conditions. The plastic strain is carried either by shear bands only, or by shear bands and deformation bands, in the specimens fatigued under strain control. Consequently, fatigue cracks nucleated either along shear bands or along deformation bands. However, the plastic strain only localized in the shear bands of the specimens under stress control, as a result, leading to shearing fatigue cracking. The fatigue fractography consists of several different zones, including fatigue crack initiation, slow, fast propagation and final fracture.
Key words:  Al-0.7%Cu alloy      cyclic softening      shear bands      
Received:  23 June 2004     
ZTFLH:  TG111.8  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I4/380

[1]Segal V M. Mater Sci Eng, 1995; A197: 157
[2]Valiev R Z. Prog Mater Sci, 2000; 45: 103
[3]Iwahashi Y, Horita Z, Nemoto M, Longdon T G. Acta Mater, 1997; 45: 4733
[4]Iwahashi Y, Horita Z, Nemoto M, Longdon T G. Acta Mater, 1998; 46: 3317
[5]Wang Y M, Chen M W, Zhou F H, Ma E. Nature, 2002; 419: 912
[6]Valiev R Z. Adv Eng Mater, 2003; 5: 296
[7]Agnew S R, Weertman J R. Mater Sci Eng, 1998; A244: 145
[8]Hoppel H W, Zhou Z M, Mughrabi H, Valiev R Z. Philos Mag, 2002; A82: 1781
[9]Wu S D, Wang Z G, Jiang C B, Li G Y. Scr Mater, 2003; 48: 1605
[10]Vinogradov A Yu, Patlan V, Hashimoto S, Kitagawa K. Philos Mag, 2002; A82: 317
[11]Vinogradov A, Nagasaki S, Patlan V, Kitagawa K, Kawa zoe M. Nanostruct Mater, 1999; 11: 925
[12]Vinogradov A, Washikita A, Kitagawa K, Kopylov V I. Mater Sci Eng, 2003; A349: 318
[13]Chung C S, Kim J K, Kim H K, Kim W J. Mater Sci Eng, 2002; A337: 39
[14]Liu S M, Wang Z G. Scr Mater, 2003; 48: 1421
[15]Vinogradov A, Hashimoto S, Kopylov V I. Mater Sci Eng, 2003; A355: 277
[16]Vinogradov A, Patlan V, Suzuki Y, Kitagawa K, Kopylov V I. Ada Mater, 2002; 50: 1639
[17]Kim H K, Choi M I, Chung C S, Shin D H. Mater Sci Eng, 2003; A340: 243
[18]Vinogradov A Y, Stolyarov V V, Hashimoto S, Valiev R Z. Mater Sci Eng, 2001; A318: 163
[19]Polmear I J. Light Alloys. Edward Arnold, 1981
[20]Mughrabi H. Plastic Deformation and Fracture of Materials. UK, Cambridge: Cambridge Press, 1993
[21]Zheng L J, Chen C Q, Zhou T T, Liu P Y, Zeng M G. Mater Charact, 2003; 49: 455
[22]Zhang Z F, Wang Z G, Sun Z M. Ada Mater, 2001; 49: 2875
[23]Li S X, Li X W, Zhang Z F, Wang Z G. Philos Mag, 2002; A82: 867
[24]Suresh S. Fatigue of Materials (2nd ed). UK, Cambridge: Cambridge Press, 1998
[1] . Fatigue Property of Ultrafine-grained Copper Produced by ECAP[J]. 金属学报, 2007, 43(5): 498-502 .
[2] SHAN Guangbin; WEI Bingchen; LI Jinxu; QIAO Lijie; CHU Wuyang. Effects of Hydrogen on Shear Bands and Cracking in Zr Base Bulk Amorphous Alloy[J]. 金属学报, 2006, 42(7): 689-693 .
[3] WU Ximao;Al Suhua;ZHANG Yun;WANG Zhonmang;HAN Xinglin (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Shenyang Polytechnic University. Shenyang 110023). THE LOW CYCLE FATIGUE BEHAVIOUR FOR 8090 Al-Li ALLOYS[J]. 金属学报, 1997, 33(7): 702-708.
[4] CHAI Huifen;RUAN Zheng;FAN Quncheng (Xi'an Jiaotong University)(Manuscript received 7 December; 1993; in revised form 10 June; 1994). SLIP BANDS OF PRESTRAINED AND CYCLED Cu AND Cu-Zn ALLOY[J]. 金属学报, 1994, 30(11): 502-506.
[5] HU Zhenhua;XIAO Jiexuan Huazhong University of Science and Technology; Wuhan HU Zhenhua; associate professor; Huazhong University of Science and Technology;Wuhan 430074. CYCLIC SOFTENING IN HOT-WORKING DIE STEELS DURING LOW CYCLE FATIGUE[J]. 金属学报, 1989, 25(6): 55-59.
[6] XIA Yuebo;WANG Zhongguang Institute of Metal Research; Academia Sinica; Shenyang XIA Yuebo; associate professor; Institute of Metal Research; Academia Sinica;Shenyang 110015. LOW CYCLE FATIGUE OF Cr-Mn-N STAINLESS STEEL[J]. 金属学报, 1989, 25(6): 37-42.
No Suggested Reading articles found!