| Time-Dependent Ratcheting Behavior of SS304 Stainless Steel Under Uniaxial Cyclic Loading at Room Temperature |
| KANG Guozheng; SUN Yafang; ZHANG Juan; KAN Qianhua |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
|
Cite this article:
KANG Guozheng; SUN Yafang; ZHANG Juan; KAN Qianhua. Time-Dependent Ratcheting Behavior of SS304 Stainless Steel Under Uniaxial Cyclic Loading at Room Temperature. Acta Metall Sin, 2005, 41(3): 277-281 .
|
|
|
Abstract The uniaxial time-dependent strain cyclic characteristics and ratcheting
behavior of SS304 stainless steel were studied by cyclic loading
experiments at room temperature. The effects of straining and stress
rates, hold time and loading chart on cyclic
softening/hardening feature and ratcheting were discussed. It is shown
that the SS304 stainless steel presents remarkable time-dependent
characteristics even at room temperature, the cyclic deformation
behaviors, especially for ratcheting, depend significantly on
strain and stress rates, holding time and loading
charts. Some significant conclusions are obtained, which is useful to
establish a constitutive model describing the time-dependent cyclic
deformation of the material.
|
|
Received: 18 May 2004
|
[1] Chaboche J L, Nouailhas D. ASME J Eng Mater Technol, 1989; 111: 384 [2] Ruggles M D, Krempl E. J Mech Phys Solids, 1990; 38: 575 [3] Delobelle P, Robinet P, Bocher L. Int J Plast, 1995; 11: 295 [4] McDowell D L. Int J Plast, 1995; 11: 397 [5] Kobayashi M, Ohno N, Igari T. Int J Plast, 1998; 14: 355 [6] Mizuno M, Mima Y, Abdel-Karim M, Ohno N. ASME J Eng Mater Technol, 2000; 122: 29 [7] Kang G Z, Gao Q, Cai L X, Yang X J, Sun Y F. Acta Metall Sin, 2000; 36: 497 (康国政,高庆,蔡力勋,杨显杰,孙亚芳.金属学报,2000; 35:497) [8] Kang G Z, Gao Q, Yang X J, Sun Y F. J Mater Sci Tech- nol, 2001; 17: 219 [9] Kang G Z, Gao Q, Cai L X, Sun Y F. Nucl Eng Des, 2002; 216: 13 [10] Kang G Z, Gao Q, Yang X J. Int J Mech Sci, 2002; 44: 1645 [11] Chaboche J L. Int J Plast, 1991; 7: 661 [12] Delobelle P. Int J Plast, 1993; 9: 65 [13] Ohno N, Wang J D. Int J Plast, 1993; 9: 375 [14] Yoshida F. Eur J Mech A-Solids, 1995; 14: 97 [15] Jiang Y, Sehitoglu H. ASME J Appl Mech, 1996; 63: 720 [16] Ohno N, Abdel-Karim M. ASME J Eng Mater Technol, 2000; 122: 35 [17] Bari S, Hassan T. Int J Plast, 2002; 18: 873 [18] Kang G Z, Gao Q, Yang X J. Mech Mater, 2002; 34: 521 [19] Gao Q, Kang G Z, Yang X J. Theor Appl Fract Mech, 2003; 40: 105 [20] Kang G Z. Mech Mater, 2004; 36: 299 [21] Kang G Z, Ohno N, Nebu A. Int J Plast, 2003; 19: 1801 |