| An Experimental Study on the Deformation Behavior of SS304 Stainless Steel UnderNonproportional Cyclic Stress and Strain at Room Temperature |
| YANG Xianjie; GAO Qing; CAI Lixun; LIU Yujie |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
|
Cite this article:
YANG Xianjie; GAO Qing; CAI Lixun; LIU Yujie. An Experimental Study on the Deformation Behavior of SS304 Stainless Steel UnderNonproportional Cyclic Stress and Strain at Room Temperature. Acta Metall Sin, 2004, 40(9): 935-942 .
|
|
|
Abstract Under several nonproportional cyclic elliptic and rhombic paths with different ratios between the
lengths of long axes and the short axes, the effects of the path shapes of the cyclic strain and cyclic stress, the
equivalent stress and strain amplitudes for the paths, the mean strain and their loading history on the
nonproportional cyclic deformation behavior were experimentally investigated for SS304 stainless steel at room
temperature. The experimental study shows that the cyclic plastic behavior of SS304 stainless steel depends
strongly on the path shapes of the cyclic strain and cyclic stress,
the equivalent stress and strain amplitudes
for the paths and their loading history.
|
|
Received: 10 October 2003
|
|
|
[1] Ikegami K, Niitsu Y. Nuclear Eng Design, 1989; 114: 355 [2] Murakami S, Kawai M, Ohmi Y. J Eng Mater Technol-Trans ASME, 1989; 111: 278 [3] McDowell D L. J Eng Mater Technol-Trans, 1985; 107:307 [4] Tanaka E, Murakami S, Ooka M. J Mech Phys Solids,1985; 33: 559 [5] Yang X J. J Eng Mater Technol-Trans ASME, 1997; 119:12 [6] Yang X J, Gao Q, He G Q, Cai L X. Ada Metall Sin,1996; 32: 15(杨显杰,高庆,何国求,蔡力勋.金属学报,1996;32:15) [7] Hassan T, Kyriakides S. Int J Plast, 1994; 10: 185 [8] Jiang Y, Sehitoglu H. Int J Plast, 1994; 10: 579 [9] McDowell D L. Int J Plast, 1995; 11: 397 [10] Delobelle P, Robinet P, Bocher L. Int J Plast, 1995; 11:295 [11] Corona E, Hassan T, Kyriakides S. Int J Plast, 1996; 12:117 [12] Yang X J, Gao Q, Cai L X, Xiang Y K. Ada Aeronaut Astronaut Sin, 1997; 18: 395(杨显杰,高庆,蔡力勋,向阳开.航空学报,1997;18:395) [13] Yang X J, Gao Q, Cai L X, Xiang Y K. Ada Mech SolidsSin, 1997; 10: 359 [14] Ohno N, Abdel-Karim M, Kobayashi M, Igari T. Int JPlast, 1998; 14: 355 [15] Bower A F. J Mech Phys Solids, 1989; 37: 455 [16] Yang X J. PhD thesis, Southwest Jiaotong University,Chengdu, 1992(杨显杰.西南交通大学博士学位论文,成都, 1992)< |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|