HOT CORROSION BEHAVIOR OF Ni--Co--Cr--Al--Y--Si--B COATING DEPOSITED BY AIP
WANG Qimin; WU Yingna; KE Peiling; JI Ailing; SUN Chao; HUANG Rongfang; WEN Lishi
State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016
Cite this article:
WANG Qimin; WU Yingna; KE Peiling; JI Ailing; SUN Chao; HUANG Rongfang; WEN Lishi. HOT CORROSION BEHAVIOR OF Ni--Co--Cr--Al--Y--Si--B COATING DEPOSITED BY AIP. Acta Metall Sin, 2004, 40(4): 399-403 .
Abstract Ni--Co--Cr--Al--Y--Si--B coatings were deposited on Ni base superalloys
DZ125 and DSM11 by arc ion plating (AIP). The corrosion behaviors of DZ125, DSM11 and Ni--Co--Cr--Al--Y--Si--B coating in molten
75%Na2SO4+25%K2SO4 at 900℃ were studied. The results indicate that the coating can protect the DZ125 and DSM11 alloys from hot corrosion destruction due to the formation of a
continuous and dense α--Al2O3$ scale. In the last stage of the hot corrosion process, the hot corrosion behaviors of base alloys have
important influences on behaviors of the whole systems.
[1] Nicholls J R, Stephenson D J. Surf Eng, 1991; 3: 156 [2] Wang F H, Lou H Y. Corros Sci Prot Technol, 1992; 4(3) :156(王福会,楼翰一.腐蚀科学与防护技术, 1992;4(3) :156) [3] Goward G W. Mater Sci Technol, 1986; 2(3) : 194 [4] Wang B, Huang R F, Gong J, Wang Q M, Liang Y, SunC, Wen L S, Han Y F. Acta Metall Sin, 2000; 36: 1094(王冰,黄荣芳,宫骏,王启民,梁越,孙超,闻立时,韩雅芳.金属学报,2000;36:1094) [5] Wang B, Wang A Y, Sun C, Huang R F, Wen L S. ChinJ Aero, 2001; 14(2) : 106 [6] Wu W T, Rahmel A, Schorr M. Oxid Met, 1983; 19(5/6) :201 [7] Zhang Y S. J Chin Soc Corros Prot, 1992; 12(1) : 1(张允书.中国腐蚀与防护学报, 1992;12(1) :1) [8] Nicoll A R, Wahl G. Thin Solid Films, 1982; 95: 21 [9] Deng X J, Zhang D H. J Chin Soc Corros Prot, 1997;17(supplement): 441(邓新建,张东辉.中国腐蚀与防护学报,1997;17(增刊):441) [10] Moon D P. Mater Sci Technol, 1989; 5: 754