Study of Manganese Oxide Reduction in Slag - Metal Phase Through Thermodynamics of Irreversible Process
ZHAI Yuchun; WANG Jinxia
School of Materials & Metallurgy; Northeastern University
Cite this article: 

ZHAI Yuchun; WANG Jinxia. Study of Manganese Oxide Reduction in Slag - Metal Phase Through Thermodynamics of Irreversible Process. Acta Metall Sin, 2004, 40(3): 305-308 .

Download:  PDF(3904KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thermodynamics of irreversible process offers linear expressions among physical quantities when there are physical--chemistry changes in the systems close to equilibrium, which has been extended to the systems far from equilibrium, and a uniform nonlinear chemical reaction rate equation was established to describe chemical reaction rate, that is in general far from equilibrium in discontinuous system, in which exist interface and chemical reactions. Finally, it was applied to manganese oxide reduction reaction and obtained a third--order expression, which well conforms to the experimental data. The thermodynamics of irreversible process after considering the high--order term can be applied to slag—metal reacting systems far from equilibrium.
Key words:  thermodynamics of irreversible process      manganese oxide reduction           
Received:  18 March 2003     
ZTFLH:  O642.1  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I3/305

[1] Xu C D, Lin R. Nonferrous Met, 1982; (1) :27(徐采栋,林蓉.有色金属,1982;(1) :27)
[2] Degroot S R, Mazur P ed, Translated by Lu A K. NonEqu(?)librium Thermodynamics. Shanghai: Shanghai Science and Technology press, 1981:166(Degroot S R,Mazur P ed.陆全康译.非平衡态热力学 上海:上海科学技术出版社,1981:166)
[3] Li P J. Geoscience, 1994; 8:88(李鹏九.现代地质,1994;8:88)
[4] Li R S Prog Biochem Biophy, 1990; 17(1) :19(李如生 生物化学与生物物理进展,1990;17(1) :19)
[5] John R, Leopoldo S G. J Phys Chem, 1989; 93:2091
[6] Li R S. J Chem Phys, 1989; 90(2) :899
[7] Zhai Y C. J Rare Earths Chin, 2000; 18:26(翟玉春 中国稀土学报,2000;18:26)
[8] Weldon L D, Robert D P. Met Trans, 1971; 2:1203
[1] CHEN Fuyi; JIE Wanqi. Study of Microsegregation In Al--Cu—Zn Ternary Alloys by Experiment and Scheil Model[J]. 金属学报, 2004, 40(6): 664-.
[2] ZHAI Yuchun; WANG Jinxia. Study of Manganese Oxide Reduction in Slag - Metal Phase Through Thermodynamics of Irreversible Process[J]. 金属学报, 2004, 40(3): 305-308 .
[3] . [J]. 金属学报, 2003, 39(9): 943-947 .
[4] . [J]. 金属学报, 2003, 39(3): 259-262 .
[5] . [J]. 金属学报, 2001, 37(1): 52-56 .
No Suggested Reading articles found!