| Effect of Stress on Bainitic Transformation in Steel |
| XU Zuyao (T. Y. Hsu) |
| School of Materials Science and Engineering; Shanghai Jiaotong |
|
Cite this article:
XU Zuyao T. Y. Hsu. Effect of Stress on Bainitic Transformation in Steel. Acta Metall Sin, 2004, 40(2): 113-119 .
|
|
|
Abstract Under the effect of stresses, the interphase energy may be reduced and probably the carbon atoms may redistribute, e.g., segregate at grain boundaries or other defects, and even the carbide may precipitate, resulting in the increase of the driving force for nucleation, in turn, marked raise of the nucleation rate and acceleration of incubation for bainitic transformation. The kinetics under stress is consistent with the kinetics model of ferrite and pearlite transformations under stress, i.e., the modified Avrami equation. Prior deformation of austenite may at first promote the bainite formation but may lead the occurrence of the mechanical stabilization of austenite at some later stage. The mechanism of the mechanical stabilization of austenite during bainite reaction may not be completely analogous with that during martensitic transformation, and it may only be the result from the hindrance of directional growth
of bainite by dislocations formed in deformation, retarding the overall
transformation kinetics. Model of the austenite mechanical stabilization
is expected to be established.
|
|
Received: 17 June 2003
|
|
|
[1] Denis S, Gautier E, Simon A, Beck G. Mater Sci Technol, 1985; 1: 805 [2] Duckworth W E. J Met, 1966; 18: 915 [3] Guarnieri G J, Kanter J J. Trans ASM, 1948; 40: 1147 [4] Howard R T, Cohen M. Trans AIME, 1948; 176: 384 [5] Radcliffe S V, Rollason E C. J Iron Steel Inst, London, 1959; 191: 56 [6] Goodenow R H, Barkalow R H, Hehemann R F. Iron Steel Inst Spec Rep No. 93, London, 1969: 135 [7] Ericsson C E, Bhat M S, Parker E R, Zackay V F. Metall Trans, 1976; 7A: 1800 [8] Ko T. J Iron Steel last, London, 1953; 175: 16 [9] Hawkins M J, Barford J. J Iron Steel Inst, London, 1972; 210: 97 [10] Cottrell A H. J Iron Steel Inst, London, 1945; 151: 93 [11] Jepson M D, Thompson F C. J Iron Steel Inst, London, 1949; 162: 49 [12] Porter L E, Rosenthal P C. Acta Metall, 1959; 7: 504 [13] Radcliffe S V, Schatz M, Kulin S A. J Iron Steel Inst, London, 1963; 201: 143 [14] Nilan T G. TMS AIME, 1967; 239: 898 [15] Drozdov B Y, Kogan L I, Entin R I. Phys Met Metallogr, 1962; 13: 135 [16] Umemoto M, Bando S, Tamura I. In: Tamura I et al eds., Proc Int Conf Martensitic Transformations 1986, Sendal, Japan: The Jpn Inst Met, 1987: 595 [17] BhadeshiaH K D H, David S A, Vitek J M, Read R W. Mater Sci Technol, 1991; 7: 686 [18] Matsuzaki A, Bhadeshia H K D H, Harade H. Acta Metall Mater, 1994; 42: 1081 [19] Shipway P H, Bhadeshia H K D H. Mater Sci Eng, 1995; A201: 143 [20] Freiwillig R, Kudrman J, Chrska P. Metall Trans, 1976; 7A: 1091 [21] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905, 1915 [22] Xu Z Y (Hsu T Y). Martensitic Transformation and Martensite. 2nd ed., Beijing: Science Press, 1999: 593, 700(徐祖耀、马氏体相变与马氏体.第2版,北京:科学出版社,1999:593,700) [23] Bhadeshia H K D H. Mater Sci Eng, 1999; A273-275: 58 [24] Bhadeshia H K D H. Bainit'e in Steels. 2nd ed., Cambridge: The Cambridge University Press, 2001: 207 [25] Tsazaki K, Ueda T, Fujiwara K, Maki T. In: Igata N, Kimpara I, Kishi T, Nakata E, Okura A, Uryn T, eds., New Materials and Processes for the Future, Proc 1st Japan Int SAMPE Symp and Exhibition, Chiba, Japan: Society for the Advancement of Materials and Process Engineering, 1989: 799 [26] Singh S B, Bhadeshia H K D H. Mater Sci Technol, 1996; 12: 610 [27] Yang J R, Huang C Y, Hsiech W H, Chiou C S. Mater Trans JIM, 1996; 37: 579 [28] Larn R H, Yang J R. Mater Sci Eng, 2000; A278: 278 [29] Lange W F Ⅲ, Enomoto M, Aaronson H I. Metall Trans, 1988; 19A: 427 [30] Hsu T Y (Xu Z Y), Mou Y W. Acta Metall, 1984; 32: 1469 [31] Brandes E A. Smithells Metals Reference Book. London: Butterworths, 1983: 15-2 [32] Grujicic M, Zhou X W. CALPHAD, 1993; 17: 383 [33] Feder J, Russell K C, Lothe J, Pound G M. Adv Phys, 1966; 15: 111 [34] Gao N, Liu Z, Yu Y P. Trans Mater Heat Treat, 2001; 22(3) : 1(高宁,刘庄,余永平.材料热处理学报,2001;22(3) :1) [35] Ye J S. PhD Thesis, Shanghai Jiaotong University, 2003(叶健松.上海交通大学博士学位论文,2003) [36] Hsu T Y (Xu Z Y), Chen W Z. Scr Metall, 1987; 21: 1289C |