Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (2): 179-183    DOI:
Current Issue | Archive | Adv Search |
RHEOLOGICAL MECHANICS MODEL OF SHEAR RATE THICKENING THE BEHMIOR OF SEMISOLID SLURRISS
CHEN Xiaoyang;MAO Weimin;ZHONG Xuegou (Institute of Casting; University of Science and Technology Beliing; Beijing 100083)
Cite this article: 

CHEN Xiaoyang;MAO Weimin;ZHONG Xuegou (Institute of Casting; University of Science and Technology Beliing; Beijing 100083). RHEOLOGICAL MECHANICS MODEL OF SHEAR RATE THICKENING THE BEHMIOR OF SEMISOLID SLURRISS. Acta Metall Sin, 1998, 34(2): 179-183.

Download:  PDF(431KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The constitutive behavior of semisolid slumes depends on a number of macroscopic factors. These factors translate to internal variables and external variables that govern the rheological behavior of the material. Internal variables include a measure of the degree of agglomeration among solid pericles, fluid phase viscosity, particle size, particle morphology, and distribution of particle sizes. External variables are temperature and shear rate. According to the different characters of semisolid slurries, we can give the corresponding new models under the different conditions on the basis of the primary models.
Key words:  shear rate thickening      semisolid slurry      rheological model     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/179

1Joly P A, Merhraian R.J Mate, Sci 1976; 11: 1393
2Flemings M C.Metall Trans A,1991;22A:957
3Ito Y,Flemings M C,Cornie J A.Nature and Properties of Semi-Solid Materials, Warrendade,PA:TEM, 1992; 3
4Rice J R,J Appl Mech,1970;9:728
5 Alers W, Overbeek J T G.J Col Sci, 1960; 15: 489
6Kumar P,Martin C L;Brown S B.Acta Metall,1994;4:3595
7Frankel N A, Acrivos A. Chem Eng Sci 1967; 22: 847
8Martin C L, Kumar P, Brown S B. Acta Metall, 1994; 42: 3603
9Nguyen T G, Favier D, Suery M. Int J Plast, 1994; 10: 693-
[1] ZHAO Junwen WU Shusen WAN Li CHEN Qihua AN Ping. EVOLUTION OF MICROSTRUCTURE OF SEMISOLID METAL SLURRY IN ULTRASOUND FIELD[J]. 金属学报, 2009, 45(3): 314-319.
No Suggested Reading articles found!