COMPUTERIZED PREDICTION OF LIQUIDUS AND SOLIDUS CURVES OF BINARY ALLOY SYSTEMS OF TRANSITION METALS WITH CONTINUOUS SOLID SOLUTIONS
GUO Jingkang;CHEN Nianyi (Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)
Cite this article: 

GUO Jingkang;CHEN Nianyi (Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050). COMPUTERIZED PREDICTION OF LIQUIDUS AND SOLIDUS CURVES OF BINARY ALLOY SYSTEMS OF TRANSITION METALS WITH CONTINUOUS SOLID SOLUTIONS. Acta Metall Sin, 1998, 34(2): 176-178.

Download:  PDF(257KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using the atomic radii, principle quantum number of valance shells, the number of d-electrons and f-electrons as the inputs of artificial neural network and trained by known data of liquidus and solidus curves, the liquidus or solidus curves of the binary alloy systems of transition metals with continuous solid solutions can be predicted correctly.
Key words:  transition metal      continuous solid solution      computerized prediction     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/176

1Chen N Y,Li C H,Yao S W Wang X Y.J Alloys Compounds, 1996;23:126,130
2Chen N Y, Li C H, Yao S W, Wang X Y.J Alloys Compounds to be published
3Li C H, Su H, Qin P, Chen N Y.J Phys Chem Solids, 1996; 75: 1797
4Guo J K, Li C H, Liu H L, Chen N Y.J Moter Sci Technol, 1997; 13: 431
5焦李成神经网络的实现与应用:西安电子科技大学出版社:1993 (Jiao L C.The Realization and Application of Neural Network, Xi'an University of Electron Science and Technology Press,1993)
6Thaddeus B, Massalshi. Binary Alloy Phase Diagrams, USA: ASM International, 1990
[1] ZHANG Xinfang; WANG Yingmin; PENG Min; WANG Qing; LI Dejun; DONG Chuang. Composition Optimization of the Zr-Al-Co Bulk Metallic Glasses[J]. 金属学报, 2004, 40(10): 1103-1103 .
[2] ZHANG Zhaochun; LI Chonghe; CHEN Nianyi (Shanghai Institute of Metallurgy;The Chinese Academy of Sciences Shanghai 200050). SOME REGULARITIES OF MONOTECTIC BINARY ALLOY SYSTEMS OF NON-TRANSITION METALS[J]. 金属学报, 1997, 33(12): 1252-1255.
[3] GUO Jin;LI Chonghe;CHEN Nianyi(Shanghai Institute of Metallurgy; Chinese Acadamy of Sciences; Shanghai 200050)(Manuscript received 1995-09-15; in revised form 1995-12-08). PLS METHOD APPLIED TO HYDROGEN STORAGE PROPERTIES OF BINARY TRANSITION METAL ALLOYS[J]. 金属学报, 1996, 32(5): 557-560.
No Suggested Reading articles found!