THE INFLUENCE OF SEVERAL FACTORS ON THE PREPARATION OF NITRIDE IRON MAGNETIC FLUID
LIU Silin;YU Yingyi;TENG Ronghou;XU Jiaoren (Central Iron and Steel Research Institute; Beijing 100081)
Cite this article: 

LIU Silin;YU Yingyi;TENG Ronghou;XU Jiaoren (Central Iron and Steel Research Institute; Beijing 100081). THE INFLUENCE OF SEVERAL FACTORS ON THE PREPARATION OF NITRIDE IRON MAGNETIC FLUID. Acta Metall Sin, 1998, 34(11): 1223-1226.

Download:  PDF(731KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influences of Fe(CO)5 thermal decomposition temperature (iron nitriding temperature), the flow of NH3 and surface activated agent on the preparation of nitride iron magnetic fluid were discussed. The result shows that the appropriate Fe(CO)5 theraml decomposition temperature is 180 to 210℃. Excessive NH3 and surface activated agent suitable to nanometer iron nitride magnetic particle and carrier liquid are necessary to preparing nitride iron magnetic with favorable property.
Key words:  nitride iron      magnetic fluid      nano particle     
Received:  18 November 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I11/1223

1 Terada N,Hoshi Y,Naoe M,Yamanaka S.IEEE Trans Magn,1984;20:1451
2 Umeda K, Kita E,Tasaki A.IEEE Trans Magn;1986;22:591
3 Miyajima H. J Magn Soc Jpn,1991;3:676
4 Nakalima K,Sato T,Okamoto S.J Magn Soc Jpn,1990; 2:77M
[1] HU Yemin,LIAN Xintong,DONG Han. On Silver Nano Particles and Silver-Bearing Materials as Virus and Bacteria Killing Agents[J]. 金属学报, 2020, 56(4): 633-641.
[2] JIAO Yuning;LIU Qingmin;YANG Yuangsheng;GE Yunlong;HU Zhuangqi(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 4 October;1993;in revised form 12 November;1993). EFFECTS OF ELECTROMAGNETIC FLUID FLOW ON Al-Al_2Cu EUTECTIC MORPHOLOGIES[J]. 金属学报, 1994, 30(6): 286-288.
No Suggested Reading articles found!