Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (7): 774-780    DOI:
Current Issue | Archive | Adv Search |
THE INFLUENCE OF DROPLET IMPACT ON METAL INERT GAS WELD POOL GEOMETRY
WU Chuansong (Shandong University of Technology; Jinan 250061); L. DORN (Berlin Technical University; Germany)
Cite this article: 

WU Chuansong (Shandong University of Technology; Jinan 250061); L. DORN (Berlin Technical University; Germany). THE INFLUENCE OF DROPLET IMPACT ON METAL INERT GAS WELD POOL GEOMETRY. Acta Metall Sin, 1997, 33(7): 774-780.

Download:  PDF(1125KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A numerical analysis model for fluid flow and heat transfer in metal inert gas (MIG) weld pools was introduced. It puts emphasis on analyzing how the droplet impact af fects the MIG weld pool geometry, and gives a set of algorithm to calculate weld reinforcement and weld pool geometry. Quantitative analysis is carried out to determine the extent of influence of droplet impact on weld pool geometry when droplet reaches the pool surface. Bead-on-plate MIG welding experiments on mild steel workpieces show that the predicted weld dimensions are in agreement with the measured ones.
Key words:  droplet impact      MIG weld pool      surface configuration     
Received:  18 July 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I7/774

1TsaoKC,WuCS.WeldJgl988;67:70—s
2 Wu C S.Eng Comput,1992;9:529
3Pardo E, Weckamn D C. Metall Trans, 1989; 20B: 937
4 TekriwalP,MazumderJ.Weld J,1988;67:150—s
5曹振宁,武传松,吴林.金属学报,1994;30:B537
6 Kim J-W,Na S-J.Trans ASME:JEnglnd,1994;116:78
7KetterRL,Prawel S R.Mode。Methods of Engineering Computation New York:McGraw—Hill,1969:38
8 Waszink J H,van den Heuvel G J P M.Weld J,1982;61:269—s
9 Essers W G,Walter R.Weld J,1981;60:37—s
10Liguo E, Wu L, Zhang J. Chin Weldg 1993; 2: 55
11 LinML,EagerTW.MetallTrans,1986;17B:601
12Smart H B. ASM Handbook. Vol.6, Metals Park, Ohio: ASM International, 1993: 25l
[1] CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology). COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT[J]. 金属学报, 1994, 30(24): 537-542.
No Suggested Reading articles found!