EVALUATION AND ANALYSIS OF THE ELECTROCHEMICAL CAPACITY OF METAL HYDRIDE ELECTRODE USING HYDROGEN STORAGE ALLOYS IN ALKALINE AQUEOUS SOLUTION
JIANG Jianjun (Huazhong University of Science and Technology; Wuhan 430074); LEI YOngquan;SUN Dalin;WU Jing;WANG Qidong (Zhejiang University; Hangzhou 310027)
Cite this article:
JIANG Jianjun (Huazhong University of Science and Technology; Wuhan 430074); LEI YOngquan;SUN Dalin;WU Jing;WANG Qidong (Zhejiang University; Hangzhou 310027). EVALUATION AND ANALYSIS OF THE ELECTROCHEMICAL CAPACITY OF METAL HYDRIDE ELECTRODE USING HYDROGEN STORAGE ALLOYS IN ALKALINE AQUEOUS SOLUTION. Acta Metall Sin, 1997, 33(7): 729-736.
Abstract To determinate an appropriate method measuring the performance of a metal hydride electrode, three different electrochemical apparatus were designed. The results showed that electrochemical capacity of hydride measured by a conventional three-electrode open cell was higher than that determined in a sandwiched and in a sealed Ni/MH test cell.The electrochemical capacity of a hydride electrode measured in a sandwiched Ni/MH cell was very close to that measured in a sealed test cell. In order to optimize the metal hydride electrode alloy and elevalute the discharge capacity of an alloy, the factors affecting the discharge process of an actual hydride electrode were examined theoretically and experimentally. It can be concluded that the electrochemical capacity of a hydride electrode depends not only on the intrinsic properties of a hydrogen storage alloy, but also on the electrode preparation method and its working environment.
1江建军,雷永泉,孙大林,吴京,王启东.稀有金属材料与工程,1993;22(3):68 2 Meli F,Zuettel A,Schlapbach L.J Alloys Compd 1993;202:81 3 Lei Y Q,Jiang J J,Sun D L,Wu J,Wang Q D.J Alloys Compd,1995;231:553 4 Sun D L,Jiang J J, Lei Y Q,Liu W D,Wu J,Wang Q D,Yang G M.Mater Sci Eng,1995;30B:19 5江建军.浙江大学博士学位论文,1995 6van Rijswick M H J.In:Andersen A F,Maeland A J eds,Proc Int Sympon the Hydride for EnergyStoragu, Gello 1977, Oxford: Pergamon Press, 1978: 261 7 YayamaH,KurlkiK,Tomodiyo A,Tomokiyo A.Jpn J Appl Phys,1986;25:739 8 Conway B E,Jerkiewica G.J Electroanal Chem,1992;326:277 9查全性.电极过程动力学.第二版,北京:科学出版社,1987:178 10王春生.浙江大学博士学位论文,1995
L Guanglie; LIU Shunhong;CHEN Linshen; WU Hongli (Hangzhuo University;Hangzhuo 310028); LEI Yongquan; YU Jinyun; YANG Xiaoguang; WANG Qidong(Zhejiang Universiyy; Hangzhuo 310027)(Manuscript received 1995-11-27). PHASE COMPOSITION STUDY FOR ZIRCONIUM-BASED PSEUDOBINARY ZrM_2(M=Ni,Mn,Cr,V)[J]. 金属学报, 1996, 32(7): 779-784.
[15]
LIN Qin; LI Rong; YE Wen; CHEN Hing (University of Science and Technology Beijing Beijing;Beijing 100083)LIU Renmin (General Research Institute of Non-Ferrous Metals Beijing; Beijing 100088). KINETICS OF HYDROGEN ABSORPTION IN ML-Ni-Co-Mn-Al ALLOYS[J]. 金属学报, 1996, 32(6): 624-628.