Abstract The solute distribution at the S/L interface is studied with stochastic dynamics. A general fuction relation between the solute distribution coefficient K and time t is given. The deviation of K from K0 (t→∞, K=K0) at the time t, being greater than the thermal equilibrium relaxation time ξ and smaller than the structural equilibrium relaxatin time ξ0, is also discussed. It has come to the conclusion that the deviation of K from K0, in K/K0, increases with increasing superheating temperature. This is in agreement with the result of experiment.
|
|
Received: 18 May 1997
|
1闵乃本.晶体生长的物理基础.上海:上海科学技术出版社,1982:49 2毛协民,傅恒志,周尧和.西北工业大学学报,1985;3(10):11 3 HφyeJ S.J Stat Phys,1987;49:297 4欧阳容百.非平衡态统计物理学.南京:南京大学出版社,1989:286 5 Van Kampen N G.Stochastic Processes in Physics and Chemistry.Amsterdam:North-Holland Publishing Company,1981:232 6王竹溪,郭敦仁.特殊函数概论.北京:科学出版社,1976:367 7谢朝阳,田荫棠,包荫鸾.西北工业大学学报,1988;6:219 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|