MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY
WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940)
Cite this article: 

WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY. Acta Metall Sin, 1997, 33(12): 1289-1294.

Download:  PDF(583KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thermomagnetic curves (σs-T curve) of Fe(72.7)Cu1Nb2V(1.8)Si(13.5)B9 alloy annealed at different temperatures (763-883 K) for 1h were investigated by magnetic analysis.Based on theσs1/8 -T curve and X-ray diffraction analysis, the changes in volume fraction,saturation magnetization and Curie temperature of α-Fe(Si) phase and residual amorphous phase with annealing temperatures as well as the correlation between them were determined.The results showed that the saturation magnetization and Curie temperature of α-Fe(Si)phase, σsαand were decreased a little with increasing of Ta when Ta< 823 K and then invariable for Ta≥823K. The saturation magnetization and Curie temperature of residual amorphous phase,σsα and TCα were all decreased monotonically with increasing of Ta in the whole annealing process and had a linear correlation between them. The dependences of magnetic coupling between α-Fe(Si) grains and of saturation magnetostriction on volume fractions of each phase were also discussed.
Key words:  Fe-Cu-Nb-V-Si-B alloy      α-Fe(Si) phase      residual amorphous phase      saturation magnetization      Curie temperature     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I12/1289

1Yoshizawa Y,Oguma S,Yamauchi K.J Appl Phys,1988;64:6044
2张延忠,年素珍,金惠娟,许桂琴,杨燮龙,李香箐.金属学报, 1995; 31: B212
3Wang Zhi,He Kaiyuan,He Shuli,Zhang Luo,Yin Jun,Zhang Yumei,Cheng Lizhi.Proceeding ofthe Ninth International Conference on Rapidly Quenched Materlals and MetastableAlloys, Bratislava, 1996
4Narita K, Yamasaki J, Fukunaga H. IEEE Trans Magn, 1980; 16: 4355
5Herzer G.IEEE Trans Magn,1989;25:3327
6He Kaiyuan, Zhou Fei, Zhi Jing, Cheng Lizhi. In: Kim C S, Lee T D, Oh J H eds.. Proceedings ofthe Third International Symposium on Physics of Magnetic Materials, Seoul, Korea: The KoreanMagnetics Society, 1995: 245
7Bozorth R M. Ferromagnetism. New York: Van Norstrand, 1951: 74
8Tebble R S, Craik D J. Magnetic Mater, 1969: 106
9oshizawa Y,Yamauchi K.Mater Sci Eng,1991;133:176
10Hasegawa R,Ray R.J Apppl Phys,1979;50:1586
11Herzer G.Mater Sci Eng,1991;133:1
12王治,何开元,贺淑莉,张玉梅,傅玉君,张洛.物理学报,1997; 46(6):134
[1] WANG Dongmei SONG Lin WANG Yaohui ZHANG Wei Bilige Tegus O. MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. 金属学报, 2011, 47(3): 344-348.
[2] Gao-Feng WANG; Lin SONG. Magnetocaloric effect on low field in non-stoichiometric MnFe(P,Si,Ge) alloys[J]. 金属学报, 2007, 43(8): 889-892 .
[3] WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY[J]. 金属学报, 1998, 34(2): 200-204.
[4] XU Hui;HE Kaiyuan;CHENG Lizhi (Department of Materials Science and Engineering; Northeast University; Shenyang 110006). MAGNETIC PROPERLIES AND STRUCTURE OF A MIXTURE OF α-Fe and Fe_3N DURING MECHANICAL ALLOYING PROCESS[J]. 金属学报, 1998, 34(1): 86-90.
[5] WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072). MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS[J]. 金属学报, 1997, 33(6): 625-630.
[6] WANG Yingung;CHEN Changpin;WANG Qidong(Zhejiang University; Hangzhou 310027); TANG Ning;YANG Fuming (State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080). STRUCTURE AND MAGNETIC PROPERTIES OF QUASI-TERNARY TbMn_(6-x)Co_xSn_6 COMPOUNDS[J]. 金属学报, 1997, 33(5): 543-547.
[7] YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x[J]. 金属学报, 1997, 33(5): 539-542.
[8] WU Ping; JIANG Enyong; LIU Yuguang; WANG Cunda(Tianjin University; Tianjin 300072). EVOLUTION OF STRUCTURE AND MAGNETIC PROPERTIES DURING CRYSTALLIZATION OF AMORPHOUS Co/Ti MULTILAYER FILMS[J]. 金属学报, 1996, 32(11): 1209-1214.
[9] YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413. NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd)[J]. 金属学报, 1993, 29(3): 84-87.
[10] ZHANG Lin; LIU Yihua(Shandong University; Jinan); WANG Hao(Dongnan University; Nanjing). STRUCTURE AND MAGNETIC PROPERTIES OF Fe/Pd COMPOSITIONALLY MODULATED FILMS[J]. 金属学报, 1992, 28(9): 77-80.
[11] CAO Lei; SHEN Baogen; YANG Linyuan; ZHAO Jiangao (State Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing). MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5) ALLOYS[J]. 金属学报, 1992, 28(11): 70-74.
[12] SHEN Baogen;ZHANG Zhiying;GUO Huiqun;ZHAO Jiangao;GU Benxi Institute of Physics; Academia Sinica; Beijing Department of Physics; Nanjing University research assistant. MAGNETIC MOMENT, CURIE TEMPERATURE AND SPIN WAVE EXCITATION FOR AMORPHOUS Fe_(90-x) Si_x Zr_(10) ALLOYS[J]. 金属学报, 1990, 26(4): 119-124.
[13] GUAN Kehong;WANG Jun Northeast University of Technology; Shenyang GUAN Kekong; associate professor; Department of Material Science and Engineering;Northeast University of Technology; 110006 Shenyang. INTRINSIC MAGNETISM AND MAGNETIC ANISOTROPY OF AMORPHOUS ALLOYS Fe_(1-x)(Si, B)_x[J]. 金属学报, 1989, 25(5): 111-114.
[14] XING Feng;JIANG Chao;HO Wenwang Department of Physics; Peking University. MAGNETIC PROPERTIES OF Nd_2(Fe_(1-x)M_x)_(14)B(M=C, Si) ALLOYS[J]. 金属学报, 1988, 24(5): 420-424.
[15] GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang. MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS[J]. 金属学报, 1988, 24(3): 296-298.
No Suggested Reading articles found!