SOME REGULARITIES OF MONOTECTIC BINARY ALLOY SYSTEMS OF NON-TRANSITION METALS
ZHANG Zhaochun; LI Chonghe; CHEN Nianyi (Shanghai Institute of Metallurgy;The Chinese Academy of Sciences Shanghai 200050)
Cite this article: 

ZHANG Zhaochun; LI Chonghe; CHEN Nianyi (Shanghai Institute of Metallurgy;The Chinese Academy of Sciences Shanghai 200050). SOME REGULARITIES OF MONOTECTIC BINARY ALLOY SYSTEMS OF NON-TRANSITION METALS. Acta Metall Sin, 1997, 33(12): 1252-1255.

Download:  PDF(383KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An extended Miedema's cellular model of alloy systems has been applied to study the regularities of binary monotectic systems consisting of non-transition metals. It has been found that larger and smaller enhance liquid--liquid immiscibility. In the three-dimensional space spanned by atomic parameters, and △Z the representative points of the non-monotectic and monotectic systems with and without solid intermetallic compounds distributed in different regions separately. The criteria of the occurrence of two layer region can be obtained by artificial neural network trained by known data of phase diagrams.
Key words:  non-transition metal      binary system      monotectic system     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I12/1252

1Miedema A R. J Less-Common Met,1973;32:117
2Chen Nianyi,Li Chonghe,Yao Shuwen,Wang Xueye.J Alloys Comp, 1996;234: 125
3Li Chonghe,Chen Nianyi.J Phys Chem Solids,(in press)
4Massalski T B, Okamoto H, Subramanian PR, Kacprzak L.Binary Alloy Phase Diagrams, SecondEdition. American Society of Metals,USA,1990
5Hugh Baker et al. ASM Handbook, Alloy Phase Diagrams.ASM International, 1992: 2
6Hanson M. Constitution of Binary Alloys. 2nd, New York: McGram—Hill, 1958: 877
7陈念贻,谢雷鸣,施天生,江乃雄,李庆芝.中国科学,1987;(7):836
8江乃雄,李庆芝,陈念贻,徐桦。中国科学,1981;(8):98
[1] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[2] CHEN Changle;LU Fuyi (Northwestern Polytechnical University; Xi'an 710072). STOCHASTIC DYNAMICS FOR NONEQUILIBRIUM SOLUTE DISTRIBUTION AT SOLID-LIQUID INTERFACE[J]. 金属学报, 1997, 33(5): 455-460.
[3] LI Bolin;ZHU Min; LI Long; LUO Kanchang;LI Zuxin (South China University of Technology; Guangzhou 510641)(Manuscript received 1996-03-19; in revised form 1996-07-15). HARDENNING AND SOFTENNING EFFECTS OF Fe-Cu NANOCRYSTALLINE SUPERSATURATED SOLID SOLUTION FORMED BY MECHANICAL ALLOYING[J]. 金属学报, 1997, 33(4): 420-426.
[4] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[5] SU Yi; WANG Zhichang(Northeastern University; Shenyang 110006). MODIFIED FORMS FOR SERIES REPRESENTATIONS OF THERMODYNAMIC PROPERTIES OF BINARY SYSTEMS[J]. 金属学报, 1995, 31(18): 255-261.
[6] DING Xueyong;WANG Wenzhong(Northeastern University;Shenyang). A NEW THERMODYNAMIC CALCULATION FORMULA FOR ACTIVITY OF COMPONENT IN BINARY SYSTEM[J]. 金属学报, 1994, 30(22): 444-447.
[7] LI Wenchao;WANG Jian;LI Xingkang;LIU Sijun(University of Scicnce and Technology Beijing); SUN Guiru(General Research Institute of Non-Ferrous Metals; Beijing). JUDGMENT OF THERMODYNAMICAL DATA AND STABILITY OF INTERMETALLIC COMPOUNDS[J]. 金属学报, 1994, 30(15): 97-103.
[8] CHEN Lili;ZHANG Kanghou Institute of Precious Metals; Kunming. PHASE DIAGRAM OF Nd-Pd(Nd≤50at.-%) BINARY SYSTEM[J]. 金属学报, 1991, 27(1): 94-97.
[9] ZHOU Ban;JIN Shiming;SHAO Jun;CHEN Nianyi Shanghai Institute of Metallurgy; Academia Sinica. EXPERT SYSTEM IMEC FOR RETRIEVAL AND PREDICTION OF BINARY INTERMETALLC COMPOUNDS[J]. 金属学报, 1989, 25(3): 137-142.
[10] YIN Dingzhen;CAO Chuan;ZHANG Yuling Institute of High Energy Physics; Academia Sinica; Beijing; Institute of Physics; Academia Sinica; BeijingHUANG Maorong Department of Apptied Research of Nuclear Technology;Institute of High Energy Physics;Academia Sinica;Beijing. STUDIES OF β-PHASE IN Co-Ga BINARY SYSTEM BY POSITRON ANNIHILATION[J]. 金属学报, 1988, 24(1): 144-146.
No Suggested Reading articles found!