INDUSTRIAL APPLICATION OF THE TECHNOLOGY PRODUCING NICKEL FOIL BY ELECTROLYSIS
ZHAO Qijin;LI RIhui;ZHAO Dehou(Beijing General Research Institute for Non-Ferrous Metals;Beijing 100088); WANG Luhong;WU Jun(Jinchuan Non-Ferrous Metals Company; Jinchang 737104)
Cite this article: 

ZHAO Qijin;LI RIhui;ZHAO Dehou(Beijing General Research Institute for Non-Ferrous Metals;Beijing 100088); WANG Luhong;WU Jun(Jinchuan Non-Ferrous Metals Company; Jinchang 737104). INDUSTRIAL APPLICATION OF THE TECHNOLOGY PRODUCING NICKEL FOIL BY ELECTROLYSIS. Acta Metall Sin, 1997, 33(11): 1194-1198.

Download:  PDF(1087KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The technology of industrial nickel foils production is researched in the present paper.The results show that the process is stable,the equipment structure is reasonable, the nickel foils produced have uniform thickness,high purity and good mechanical and apparent performance.
Key words:  nickel sulfate solution      cathode drum      electrolysis      nickel foil     
Received:  18 November 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I11/1194

1WatsonSA.TransInstMetFinish,1989;67(4):89
2赵奇金,李日辉,赵德厚,张碧田,崔鸿玉.有色金属(冶炼),1993;(3):19
[1] Jing GUO,Hanjie GUO,Keming FANG,Shengchao DUAN,Xiao SHI,Wensheng YANG. Morphology Prediction Theory and Experimental Measurement for the Secondary Phase Particle in Steel[J]. 金属学报, 2017, 53(7): 789-796.
[2] ZHAO Bingjian LU Xionggang LI Chonghe ZHONG Qingdong. DIRECT ELECTROCHEMICAL REDUCTION OF NiO–CeO2 POWDER FOR PREPARATION OF CeNi5 ALLOY BY SOLID–OXYGEN–ION
CONDUCTING MEMBRANE PROCESS
[J]. 金属学报, 2009, 45(10): 1255-1260.
[3] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
[4] ;. EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD[J]. 金属学报, 2008, 44(10): 1243-1246 .
[5] ;. A NOVEL TECHNOLOGY TO PRODUCE METAL TANTALUM DIRECTLY FROM Ta2O5[J]. 金属学报, 2006, 42(5): 500-504 .
[6] LIU Guankun; TONG Yexiang;HONG Huichan; CHEN Shengyang;GAN Luo(Zhongshan University; Guangzhou 510275)(Manuscript received 1995-10-23; in revised form 1996-08-25). STUDIES ON THE PREPARATION OF Dy-Cu ALLOY IN CHLORIDE MELT BY MOLTEN SALT ELECTROLYSIS[J]. 金属学报, 1996, 32(12): 1252-1257.
No Suggested Reading articles found!