| ACOUSTIC EMISSION MEASUREMENT OF INTERFACE SHEAR STRENGTH OF SiC_w/ Al COMPOSITE |
| ZHU Zuming; SHI Nanlin; WANG Zhongguang; LIANG Yong (State Key Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
ZHU Zuming; SHI Nanlin; WANG Zhongguang; LIANG Yong (State Key Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). ACOUSTIC EMISSION MEASUREMENT OF INTERFACE SHEAR STRENGTH OF SiC_w/ Al COMPOSITE. Acta Metall Sin, 1996, 32(9): 998-1002.
|
|
|
Abstract The model specimen of SiC_w/Al composite is subjected to the tensile test, simultaneously, the acoustic emission (AE) characteristics during the process of strain and fracture are monitered. The broken number of SiC fiber and the segment length of the broken fibers in the composite can be measared by AE technique. The interfacial shear strength and the fractural strength of fiber can be easily determined.
|
|
Received: 18 September 1996
|
| 1ChamisCC.In:PlueddemannEPed.,InterfacesinPolymerMatrixComposites,NewYork:AcademicPress,1974:312OchiaiS,MurakamioY.JMaterSci.1979;14:8313OchiaiS,MurakumioY.ZMetallk,1981;72:8274EvansAC,LuMC,ScbmauderS,RuhleM.ActaMetall,1986;34:16435ChuaPS,PiggottMR.ComposSciTechnol,1985;22:336ChuaPS,PiggottMR.ComposSciTechnol,1985;22:1857NetraveliAN,TopoleskiLT,SachseWH,PhoenixSL.ComposSciTechnol,1989;35:138CloughRB,BiancanielloFS,WadleyHNG,KattnerUR.MetallTrans,1990;20A:27479ManorA,CloughRB.ComposSciTechnol,1992;45:7310朱祖铭,石南林,王中光,粱勇.金属学报,1996:32(9):100311NetravaliAN,HenstenburgRB,PhoenixSL,SchwartyP.PolymerCompos,1989;10:22612DrzalLT,RichMJ,LloydPF.JAdhe.1983;16:113DrzalLT,RichMJ,KoenigMF,LloydPF.JAdhes,1983;16:133 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|