Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (7): 705-710    DOI:
Current Issue | Archive | Adv Search |
SURFACE LAYER STRUCTURE OF PURE IRON TREATED BY ION-RE-NITRIDATION
WU Yaqiao; YANG Lin; ZHAO Zhongjian; GAO Lifeng;XU Yongbo; LU Zhenjia (Polytechnic University; Shenyang 110023)(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-12-12)
Cite this article: 

WU Yaqiao; YANG Lin; ZHAO Zhongjian; GAO Lifeng;XU Yongbo; LU Zhenjia (Polytechnic University; Shenyang 110023)(Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-12-12). SURFACE LAYER STRUCTURE OF PURE IRON TREATED BY ION-RE-NITRIDATION. Acta Metall Sin, 1996, 32(7): 705-710.

Download:  PDF(499KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An investigation has been made on the microstructure of the surface layer in pure iron ion-nitrided with RE(rare earth) ions (Ce~+, La~+). Analysis by EPMA shows that the peak value of distribution of nitrogen element inside the pure iron with ion RE-nitridation is about 100 μm deeper than that with ion nitridation. Investigations by SAED and HRTEM show that the γ'(Fe_4N) phase exists as the uncomplete 6H type long period structure due to the effect of RE elements. There is a near K-S orientation relationship between a-Fe and γ' phase. The RE elements also exist as intermetallic compound (Ce, La)Fe_7which has approximate orientation relationship with α-Fe as follows: Correspondent: WU Yaqiao, Laboratory of Aiomic Imaging of Solids, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015
Key words:  pure iron      RE element      nitrogen element      ion-RE-nitridation      structure of surface layer     
Received:  18 July 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I7/705

1余景生,余宗森.见:余宗森主编,稀土在钢铁中的应用,北京:冶金工业出版社,1987:12 吕振家,吕其岗.见:余宗森主编.稀土在钢铁中的应用,北京:冶金工业出版社,1987:3603 孙东升,李凤照,张保荣.金属热处理学报,1992,9:464 GerardinD.MenMemSciRev,Metall.1977;74:4575 郑经,王育烽,沈甫法,余德刚,毛树楷.金属学报,1985;21:A2336 顾文桂,周天健.金属热处理学报,1990;11(4):437MichelH,CzerwiecT,GantoisM,AblitzerD,RicardA.SurfCoatTechnol,1995;72:1038HaywoodBC.HeatTreating.1991;3:119LIZhonghou,SUYunan,LIUXiaoping,XUZhong.ActaMetallSin(EngLett),1995,8:14510 BellT,KinaliM,MunstermannG.HeatTreatMet.1987;2:4711吴亚桥,杨林,赵忠俭,高丽峰,徐永波,吕振家.金属学报,1996;32:594H
[1] ZHANG Ke; NIU Yan; WU Weitao. CORROSION OF PURE IRON AND TWO COMMERCIAL STEELS BENEATH ZnCl2-KCl DEPOSITS IN A CONTROLLED ATMOSPHERE CONTAINING HCl AT 500℃[J]. 金属学报, 2004, 40(4): 388-392 .
[2] WU Yaqiao; YANG Lin; ZHAO Zhongjian; GAO Lifeng XU Yongbo; LU Zhenjia(Shenyang Polytechnic University; Shenyang 110023) (Laboratory; of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy; of Sciences; Shenyang 110015)(State Key Laborutory for Fatigue and Fracture of Materials; Institute of MetalResearch; Chinese Academy of Sciences; Shenyang 110015). A STRUCTURAL OBSERVATION ON IONIZED RE METALLIZING LAYER OF PURE IRON[J]. 金属学报, 1996, 32(6): 594-598.
No Suggested Reading articles found!