Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (7): 695-699    DOI:
Current Issue | Archive | Adv Search |
FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY
WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18)
Cite this article: 

WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18). FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY. Acta Metall Sin, 1996, 32(7): 695-699.

Download:  PDF(429KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fe_3Al alloys in B2 structure with different order degree are studied by means of field-ion microscope (FIM). Whether or not the maximum B2 order degree got, the total regularity of the FIM image is so poor that it is even difficult to know the B2 order degree qualitatively. However, the local evaporation characters of the〈100〉pole contain the information of B2 ordering. By successive examination, it is discovered that the evolution of B2 ordering is not homogeneous in nano-scale. The result got from the〈120〉pole is the similar to that from the〈100〉pole. This consistence confirms once more the conclusion"only the Al atoms contribute to the image while the Fe atoms are invisible" .Correspondent: ZHI Rentao, professor, Deportment of Materials Physics, University of Science and Technology Beijing, Beijing 100083
Key words:  Fe_3Al      FIM      ordering     
Received:  18 July 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I7/695

1SouthworthHN,RalphB.PhilMag,1970;21:232TauntRJ,SinclairT,RalphB.PhysStatSolA,1973;16:4693KrauseHJ,WittigJE,FrommegerG.ZMetallkd,1987;78:5764WengJ,ZhuFW,XiaoJM.ZMetallkd,1994;85:4325MarcinkowskiMJ,BrownN.JApplPhys,1962;33:5376NewmanRW,HrenJJ.PhilMag,1967;16:2117LinY,ZhuF,XiaoJ.AclaMetallMater,1994;42:2499^
[1] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[2] Rui YANG,Yan PAN,Wei CHEN,Qiaoyan SUN,Lin XIAO,Jun SUN. DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. 金属学报, 2016, 52(2): 135-142.
[3] Yuanke MO,Zhihao ZHANG,Jianxin XIE,Hongjiang PAN. EFFECTS OF RECRYSTALLIZATION ON THE MICROSTRUCTURE, ORDERING AND MECHANICALPROPERTIES OF COLD-ROLLED HIGH SILICON ELECTRICAL STEEL SHEET[J]. 金属学报, 2016, 52(11): 1363-1371.
[4] ZHAO Yan CHEN Zheng WANG Yongxin HUO Jinliang ZHANG Lipeng ZHANG Mingyi . A MICROSCOPIC PHASE–FIELD STUDY FOR THE INFLUENCE OF ORDERING ENERGY ON Cr SUBSTITUTION BEHAVIOR IN Ni75Al15Cr10 ALLOY[J]. 金属学报, 2009, 45(5): 635-640.
[5] WU Erdong GUO Xiumei SUN Kai. NEUTRON DIFFRACTION STUDY OF DEUTERIUM OCCUPANCY OF DEUTERIDE OF LAVES PHASE ALLOY Ti0.68Zr0.32MnCrD3.0[J]. 金属学报, 2009, 45(5): 513-518.
[6] ZHANG Xinghua; LI Zhiqing; JIANG Enyong. INFLUENCE OF La DOPING ON THE STRUCTURE,MAGNETIC AND ELECTRICAL TRANSPORT PROPERTIES OF Pr0.75Na0.25MnO3[J]. 金属学报, 2006, 42(9): 974-978 .
[7] LI Zhiqiang;REN Dagang;LI Douxing; GUO Jianting (Laboratory of Atom Imaging of Solids; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015). MICROSTRVCTURAL STUDY OF INTERMETALLIC COMPOUND Ni_3Al BY AP-FIM[J]. 金属学报, 1998, 34(3): 249-254.
[8] YU Xinquan;SUN Yangshan;MEI Jianping;SUN Guoxiong (Department of Materials Science and Engineering;Southeast University; Nanjing 210096). ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS[J]. 金属学报, 1998, 34(11): 1126-1130.
[9] ZHENG Weiwei;YANG Wangyue;LIU Qing;SUN Zuqing(Department of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083). ROOM TEMPERATURE MECHANICAL BEHAVIOR OF B2-ORDERED Fe_3Al SINGLE CRYSTALS[J]. 金属学报, 1998, 34(11): 1137-1142.
[10] SUN Yangshan;YU Xinquan;HUANG Haibo;SUN Guoxiong (Department of Materials Science and Engineering; Southeast University; Nanjing 210096). OXIDATION RESISTANCE OF Fe_3Al INTERMETALLICS AT HIGH TEMPERATURES[J]. 金属学报, 1998, 34(11): 1131-1136.
[11] ZHANG Zhonghua; SUN Yangshan; LIU Guijun (Southeast University; Nanjing 210096). IMPROVEMENT OF ROOM TEMPERATURE ENVIRONMENTAL BRITTLEMENT OF Fe_3Al-BASED ALLOY BY ELECTRO-BRUSH PLATING[J]. 金属学报, 1996, 32(9): 955-958.
[12] YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05). NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. 金属学报, 1996, 32(8): 799-804.
[13] ZHAO Zhongtao; LIU Tao; MA Ruzhang (University of Scicnce and Technology Beijing; Beijing 100083); MA Changying (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 ). ON THE PRECIPITATE IN Fe-28Al ALLOY[J]. 金属学报, 1996, 32(6): 585-588.
[14] WENG Jun; ZHU Fengwu; WANG Wendong; ZHI Rentao; ZHANG Dezhi;XIAO Jimei (University of Science and Technology Beijing; Beijing 100083). FIM STUDY ON (D0)3 ORDERING IN Fe3Al ALLOY[J]. 金属学报, 1996, 32(11): 1154-1158.
[15] ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05). HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al[J]. 金属学报, 1995, 31(7): 300-303.
No Suggested Reading articles found!