Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (6): 669-672    DOI:
Current Issue | Archive | Adv Search |
DETERMINATION OF ENTHALPY AND MASSIC HEAT CAPACITY OF SELF-BAKING CARBON BLOCK
XUE Xiangxin; CHE Yinchang (Northeastern University; Shenyang 110006)DU Yingmin (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)HUANG Hiaoyu (Ironmaking Works; Anshan Iron and Steel Company; Anshan 114012)
Cite this article: 

XUE Xiangxin; CHE Yinchang (Northeastern University; Shenyang 110006)DU Yingmin (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)HUANG Hiaoyu (Ironmaking Works; Anshan Iron and Steel Company; Anshan 114012). DETERMINATION OF ENTHALPY AND MASSIC HEAT CAPACITY OF SELF-BAKING CARBON BLOCK. Acta Metall Sin, 1996, 32(6): 669-672.

Download:  PDF(238KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Enthalpy change, △H, of partially graphitized self-baking carbon block with different graphitization degree has been determined by means of copper calorimeter in temperature range from 14 to 1000℃. It seems that the graphitization degree is not influential to △H of the carbon blocks in the range of the experimental temperature. The temperature dependence of the A△ is expressed as follows:△H=-33.31+1.11T+3.69×10~(-4)T~2+9.85×10~2Ta~(-1) By differential the temperature dependence of the massic heat capacity c_p is repesented as follows:c_P=1.11+7.38×10~(-4)-9.85×10~2T~(-2)
Key words:  self-baking carbon block      enthalpy      massic heat capacity      calorimeter     
Received:  18 June 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I6/669

1郝运中,陈前婉.炼铁,1994:13(增刊):72HaoYZ,ChenQW.ChinRefract,1994;1:93张殿友,肖亦芹,郝运中,陈前婉.炼铁,1994;13(增刊):284CarslowHS.JaegerJC.ConductionHeatinSolids,London:OxfordPress,1959:1015薛向欣,段培宁,黄晓煜,张殿有.中国科协第二届青年学术年会卫星会议辽宁省第二届青年学术会议论文集,工科分册,大连:大连理工大学出版社,1995:906姚广春.冶金炭素材料性能及工艺.北京:冶金工业出版社,1992:1997中国金属学会,中国有色金属学会编.金属材料物理性能手册(第一册).北京:冶金工业出版社,1987:2728重见彰利.制铁东京:地人书馆,1979:163
[1] Huijin TAO,Shan ZHOU,Yu LIU,Jian YIN,Hao XU. Point Defect Concentrations and Interactions in D019-Ti3Al from First-Principles Calculations[J]. 金属学报, 2017, 53(6): 751-759.
[2] ZHANG Fengying TAN Hua CHEN Jing LIN Xin HUANG Weidong. INFLUENCE OF MIXING ENTHALPY ON THE MICROSTRUCTURE OF LASER MULTILAYER DEPOSITED Ti–6Al–4V ALLOY[J]. 金属学报, 2012, 48(2): 159-163.
[3] HU Xiaojun (Department of Physicochemistry; University of Science and Technology; Beijing 100083)XUE Xiangxin; DUAN Peining (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)HUANG Xiaoyu(Ironmaking Work; Anshan Iron & Steel Company; Anshan 114021). PERMEATION PROCESS OF MOLTEN IRON IN A SELF-BAKING CARBON BLOCK[J]. 金属学报, 1998, 34(4): 384-387.
[4] XUE Xiangxin (Northeastern University; Shenyang 110006); HUANG Xiaoyu (Ironmaking Works; Anshan Iron and Steel Complex; Anshan 114021); DU Yingmin(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZHANG Dianyou(Ironmaking Works; Anshan Iron and Steel Complex;Anshan 114021). THERMAL DIFFUSIVITY OF SELF-BAKING CARBON BLOCK WITH DIFFERENT GRAPHITIZATION DEGREES[J]. 金属学报, 1996, 32(11): 1227-1232.
[5] YU Hualong;ZHU Jiankang;WANG Zhichang Northeast University of Technology; Shenyang Correspondent; professor; Department of Non-Ferrous Metallurgy; Northeast University of Technology; Shenyang 11006. ENTHALPIES OF MIXING FOR PbCl_2-NaCl-BaCl_2 TERNARY MOLTEN SALT MIXTURES[J]. 金属学报, 1992, 28(5): 90-92.
[6] LIU Huanming;YANG Zupan;TIAN Yanwen The Steel Works No.2; Benxi Iron and Steel Company Northeast University of Technology; Shenyang LIU Huanming; assistant engineer; the Laboratory of Steel Works No.2; Benxi Iron and Steel Company; Benxi; Ltaoning. SELF-REACTION COEFFICIENTS OF Ca AND Mg IN LIQUID Sn[J]. 金属学报, 1989, 25(5): 79-84.
[7] FANG Zheng;CHEN Xinmin (H. M. Chen) Central South University of Technology; ChangshaFANG Zheng;Dr.and Lecture;Department of Chemistry Cental-South Universisy of Thechnology;Changsha. EQUILIBRIUM BETWEEN NONSTOICHIOMETRIC Mo AND MoO_2——WITH APPLICATION OF SIEVERTS' LAW CONSTANT TO SMILTENS' INTEGRATION[J]. 金属学报, 1988, 24(1): 111-113.
No Suggested Reading articles found!