PLS METHOD APPLIED TO HYDROGEN STORAGE PROPERTIES OF BINARY TRANSITION METAL ALLOYS
GUO Jin;LI Chonghe;CHEN Nianyi(Shanghai Institute of Metallurgy; Chinese Acadamy of Sciences; Shanghai 200050)(Manuscript received 1995-09-15; in revised form 1995-12-08)
Cite this article: 

GUO Jin;LI Chonghe;CHEN Nianyi(Shanghai Institute of Metallurgy; Chinese Acadamy of Sciences; Shanghai 200050)(Manuscript received 1995-09-15; in revised form 1995-12-08). PLS METHOD APPLIED TO HYDROGEN STORAGE PROPERTIES OF BINARY TRANSITION METAL ALLOYS. Acta Metall Sin, 1996, 32(5): 557-560.

Download:  PDF(267KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The partial least square(PLS) method is applied to the formability of hydride and hydrogen storage properties of binary transition metal alloys. The results show that the mathematical model describing the formation of hydrogen storage materials of binary transition metal alloys can be built by using chemical bond parameters and pattern recognition method, which is useful for hydrogen storage materials design.
Key words:  transition metal      hydrogen storage property      partial least square method     
Received:  18 May 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I5/557

1VanMalHH.PhilipsResRepSuppl,1976;1:612BuschowKHJ,BoutenPCP,MiedemaAR.RepProgPhys,1982;45:9373GeladiP,KowaskiBP.AnalChimActa,1986;1:1854HoskuldssonA.JChemoetrics,1988;2:2115PearsonWB.BinaryAlloyPhaseDiagrams.NewYork:Wiley-Interscience,19726BechmanCA.DoudyA,TakeshitaT,WallaceWE.InorgChem,1976;2184:157KiersteadHA.JLess-CommonMet.1980;73:61
[1] WANG Yang; ZHANG Yan; WANG Xinhua; CHEN Changpin. HYDROGEN STORAGE PROPERTIES AND CRYSTAL STRUCTURE OF Ti-Cr BASED ALLOYS[J]. 金属学报, 2006, 42(6): 641-646 .
[2] JIANG Weiqing; HUANG Cunke; HUANG Dan; JIAN Xiaoling; GUO Jin. PLS Method Applied to Analysis of Binary Laves Phase Structures[J]. 金属学报, 2005, 41(1): 19-.
[3] ZHANG Xinfang; WANG Yingmin; PENG Min; WANG Qing; LI Dejun; DONG Chuang. Composition Optimization of the Zr-Al-Co Bulk Metallic Glasses[J]. 金属学报, 2004, 40(10): 1103-1103 .
[4] GUO Jingkang;CHEN Nianyi (Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050). COMPUTERIZED PREDICTION OF LIQUIDUS AND SOLIDUS CURVES OF BINARY ALLOY SYSTEMS OF TRANSITION METALS WITH CONTINUOUS SOLID SOLUTIONS[J]. 金属学报, 1998, 34(2): 176-178.
[5] ZHANG Zhaochun; LI Chonghe; CHEN Nianyi (Shanghai Institute of Metallurgy;The Chinese Academy of Sciences Shanghai 200050). SOME REGULARITIES OF MONOTECTIC BINARY ALLOY SYSTEMS OF NON-TRANSITION METALS[J]. 金属学报, 1997, 33(12): 1252-1255.
[6] AO Ming;WANG Qidong zhejiang University; Hangzhou Department of Materials Science;Zhejiang University;Hangzhou 310013. HYDROGEN STORAGE PROPERTIES OF Mg MODIFIED BY TETRAHYDROFURAN[J]. 金属学报, 1990, 26(3): 40-43.
[7] YANG Minjie;CHEN Bingzhao Shanghai Institute of Metallurgy; Academia Sinica. SEPARATION AND CONCENTRATION OF Kr AND Xe FROM HYDROGEN USING TiFe_(0.86)Mn_(0.1) ALLOY[J]. 金属学报, 1988, 24(2): 194-198.
No Suggested Reading articles found!