Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (3): 274-277    DOI:
Current Issue | Archive | Adv Search |
MOLTEN SALT ELECTROPLATING OF Al-Ti AND Al-Mn ALLOYS
GUO Naiming(Institute of Chemical Metallurgy; Chinese Academy of Sciences; Beijing 100080); GUO Jiaju(University of Science and Technology Beijing; Beijing 100083) (Manuscript received 1 995-07-2 1 ; in revised form 1 995- 1 0- 1 3)
Cite this article: 

GUO Naiming(Institute of Chemical Metallurgy; Chinese Academy of Sciences; Beijing 100080); GUO Jiaju(University of Science and Technology Beijing; Beijing 100083) (Manuscript received 1 995-07-2 1 ; in revised form 1 995- 1 0- 1 3). MOLTEN SALT ELECTROPLATING OF Al-Ti AND Al-Mn ALLOYS. Acta Metall Sin, 1996, 32(3): 274-277.

Download:  PDF(323KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of the ion concentration in molten salt, agitation etc. on the chemical composition, structure and surface of alloy plating were explored. The main effect on the chemical composition of alloy plating is the metal ion concentration in the molten salt. Agitation is an important condition to obtain smooth and dense plating. Electrochemical examination and corrosion test showed that the Al-Ti and Al-Mn alloy platings have excellent corrosion resistance. Correspondent: GUO Naiming, associate professor, Institute of Chemical Metallurgy, Chinese Academy of Sciences, Beijing 100080
Key words:  Al-Ti alloy      Al-Mn alloy      molten salt electroplating     
Received:  18 March 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I3/274

1 Li qingfen, Hjuler H A, Bery R W, Bjerrum N J. J Electrochem Soc, 1990; 137: 593
2 郭乃名,过家驹.表面保护技术论文集,中国腐蚀与防护学会表面保护技术专业委员会编,1993: 116
3 Guo Naiming, Guo Jiaju, Lei Jianpo. In: Zhu Rizhang ed., 95'Int Conf S:}rface Science and Engineering, Beijing> China> International Academic Publishers 1995: 201
4 Stafford G R. J Electrochem Soc. 1989; 136: 635
[1] Xiancui LIU, Ye PAN, Zhijiao TANG, Weiqiao HE, Tao LU. Microstructure Control and High Temperature Properties of Al-Mn-Based Alloys[J]. 金属学报, 2017, 53(11): 1487-1494.
[2] YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel: (010)62333436; Fax: (010)62332336. PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RSCRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅱ. Interaction Between Particles and Other Nucleation Sites and the Formation of Recrystallization Texture[J]. 金属学报, 1998, 34(8): 793-801.
[3] YANG Ping; O.ENGLER(Institute of Metal Science and Metal Physics; Aachen University of Technology; Kopernikusstr. 14; D-52056;Aachen; Germany) Now: School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing;100083 Now: Los Alamos National Laboratory; Center for Materials Science; K765; Los Alamos; NM87545; USACorrespondent: YANG Ping; Tel. (010)623s3Js6; Fax: (010)62332336. PARTICLE STIMULATED NUCLEATION AND THE FORMATION OF RECRYSTALLIZATION TEXTURE IN Al-Mn ALLOY CONTAINING PARTICLES Ⅰ. Deformation Zones Around Particles and Particle Stimulated Nucleation[J]. 金属学报, 1998, 34(8): 785-792.
[4] FAN Chuanguang;ZHANG Meng Jiangxi University; Structure Research Laboratory; University of Scieace and Technology of China; Academia Sinica; Hefei; WANG Yuansheng; WU Ziqin University of Science and Technology ol China; Hefei. SOME FRACTAL STRUCTURES IN RAPIDLY SOLIDIFIED Al-Mn ALLOY[J]. 金属学报, 1991, 27(6): 60-63.
[5] HAN Ming;CHEN Fumin;CHEN Jinming;CHEN Yuru;LIU Wenxi Tianjin University professor;Department of Material Science and Engineering;Tianjin University; Tianjin 300072. MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY[J]. 金属学报, 1990, 26(2): 5-9.