^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM
LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006)
Cite this article: 

LI Juntao; HAO Shiming (Northeastern University; Shenyang 110006). ^^α(α_2)/ PHASE EQUILIBRIA IN Ti-Al-Si SYSTEM. Acta Metall Sin, 1996, 32(11): 1171-1176.

Download:  PDF(438KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The partial α(α2)/γ phase equilibria in Ti-Al-Si ternary system at low Si concentration were measured by EPMA and examined with thermodynamic analysis. The results show that the addition of Si in Ti-Al binary system results in the α(α2)/ (α(α2)+γ) phase boundary shifting to Ti-rich side, whereas the (α(α2)+γ/γ) phase boundary shifting little. Si has effect on refining lamellar microstructure and makes the lamellae coarsen difficultly. The Si solubility in α(α2) phase is higher than that in γ phase thereas Si is an αphase-forming element in Ti-Al binary system. A third phase Ti5Si3 appears in the system with Si addition up to 1 .0% (atomic fraction). Correspondent: LI Juntao, Department of Materials Science and Engineering, Northeastern University.Shenyang 110006
Key words:  Ti-Al-Si ternary system      partial vertical section      α(α_2) / γ phase equilibrium     
Received:  18 November 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I11/1171

1KimYW.ActaMetallMater,1992;40:11212KimYW.JOM,1994;46(7):303TsuyamaS,MitaoS,MinakawaK.MaterSciEng,1992;A153:4514加藤哲男,草加藤司.粉体粉末冶金,1989;36(7):305DimidukDM,MiracleDB,KimYW,MendirattaMG.ISIJInt,1991;31:12236RamanujanRV.ActaMetallMater,1994;42:23137郝士明,韩传玺,吴文涛.金属学报,1993;29:A498秦高梧,郝士明.东北大学学报,1996;17:266v
[1] QIN Gaowu;HAO Shiming;ZENG Ninghua (Northeastern University;Shenyang 110006)(Manuscript received 1994-11-04;in revised form 1995-05-04). α(α_2)/γ PHASE EQUILIBRIA IN Ti-Al-Ga AND Ti-Al-Nb-Cr SYSTEMS[J]. 金属学报, 1995, 31(23): 484-488.
No Suggested Reading articles found!