| EFFECT OF Ni_3Al CONTENT ON COMBUSTION SYNTHESIS OF Ni_3Al/TiC COMPOSITES |
| MEI Bingchu;FU Zhengyi;WANG Weimin;YUAN Runzhang(Sino-Russia Research Centre for SHS;Wuhan University of Technology;Wuhan 430070)(Sino-Russia Research Centre for SHS;Wuhan University of Technology;Wuhan 430070)(Manuscript received 1995-12-25;in revised form 1996-05-27) |
|
Cite this article:
MEI Bingchu;FU Zhengyi;WANG Weimin;YUAN Runzhang(Sino-Russia Research Centre for SHS;Wuhan University of Technology;Wuhan 430070)(Sino-Russia Research Centre for SHS;Wuhan University of Technology;Wuhan 430070)(Manuscript received 1995-12-25;in revised form 1996-05-27). EFFECT OF Ni_3Al CONTENT ON COMBUSTION SYNTHESIS OF Ni_3Al/TiC COMPOSITES. Acta Metall Sin, 1996, 32(10): 1107-1110.
|
|
|
Abstract The process that Ni3Al/TiC composites were synthesized by the thermal explosion mode of self-propagating high-temperature synthesis(SHS) from Ti-C-Ni-Al system was studied.The occurrence of thermal explosion depends on two factors,one is the heating rate,and the other the heat of the system(that is,Ni3Al content).The density of the products varies with Ni3Al content,and a maximum value of density appears at 40% Ni3Al.The effect of Ni3Al content on the microstructure of the products was characterized by means of SEM technique.
|
|
Received: 18 October 1996
|
| 1FengHJ,HunterKR,MooreJJ.JMaterSynthProcess,1994;2(2):712冯长根.热爆炸理论学. 第一版,北京:科学出版社,198:33 ChoiY,RheeS-W.J MaterSci,1993;28:66694 梅炳初. 武汉工业大学博士学位论文,19955 RogachevA A,MukasyanAS.DoklAkadNaukSSSR,1987;297:14256YiHC,PetricA,MooreJJ.JMaterSci,1992;27:6797 |
| No Suggested Reading articles found! |
|
|