| INDENTATION MEASUREMENT ON HARDNESS DISTRIBUTION WITH A SINGLE LOADING-DISPLACEMENT CURVE |
| HOU Genliang; LIU Junhai; XU Kewei(State Laboratory.for Mechanical Behaviourof Materials; Xi'an Jiaotong University; Xi'an 710049) |
|
Cite this article:
HOU Genliang; LIU Junhai; XU Kewei(State Laboratory.for Mechanical Behaviourof Materials; Xi'an Jiaotong University; Xi'an 710049). INDENTATION MEASUREMENT ON HARDNESS DISTRIBUTION WITH A SINGLE LOADING-DISPLACEMENT CURVE. Acta Metall Sin, 1995, 31(5): 236-240.
|
|
|
Abstract A method calculating the hardness distribution in a whole indentation depth with a single load-placement curve was proposed. The theory is based on the experimental results that the loading pattern keeps constant and the initially unloading slope is proportion to the indention depth. This is applicable to study the hardness distribution at the surface layer of a bulk material. Both theoretical and experimental results agree well.
|
|
Received: 18 May 1995
|
| 1何家文,王宏伟,南俊马.FatigueFractEngMaterStruct,1993;16:5912BullSJ,PageTF,YotteEH.PhilosMagLett,1989;59:2813WuTW,MoshrefM,AlexopoulosPS.ThinSolidFilms,1990;187:2954VancoilleE,CelisJP,RoosJR.ThinSolidFilms.1993;224:1685FleckNA,MullerGW,AshbyMF,HutchinsonJW.ActaMetallMater,1994;42:4756SakaiM.ActaMetallMater.1993;41:17517蔡洵,张兮,周平南.理化检验(物理分册),1993;29(4):198DoernerMF,NixWD.J MaterRes、986;1:6019OliverWC,PharrGW.JMaterRes,1992;7:156410HendrixBC,刘军海,何家文.第五届全国固体薄膜会议论文集,1994:20311KingRB.IntJSolidStruct,1987;23:165712HendrixBC.JMaterRes,1995;tobepublished13PivinJC.ThinSolidFilms,1993;229:83 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|