EFFECT OF CeO_2 DISPERSION ON INITIAL STAGE GROWTH OF α-Al_2O_3 OXIDE SCALE AT HIGH TEMPERATURE
MA Xinqing; LI Meishuan; PENG Hiao; CHEN Quanfang; LI Tiefan (State Key. Laboratory; of Corrosion and Protection; Inslitute of Corrosion and Prolection of Metals;Chinese Academy; of. Sciences; Shenyang 110015)(Manuscript received 1995-01-10; in revised form 1995-06-06)
Cite this article: 

MA Xinqing; LI Meishuan; PENG Hiao; CHEN Quanfang; LI Tiefan (State Key. Laboratory; of Corrosion and Protection; Inslitute of Corrosion and Prolection of Metals;Chinese Academy; of. Sciences; Shenyang 110015)(Manuscript received 1995-01-10; in revised form 1995-06-06). EFFECT OF CeO_2 DISPERSION ON INITIAL STAGE GROWTH OF α-Al_2O_3 OXIDE SCALE AT HIGH TEMPERATURE. Acta Metall Sin, 1995, 31(21): 399-405.

Download:  PDF(567KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the base of studying morphologies and compositions of the a-AlaO3 scales formed on the NiAl bases with CeO2 dispersion during initial oxidation stage at 1000 and 1100℃, the effect of the dispersive CeO2 in the NiAl base on the element diffusion flux in surface zone was analysized. According to the analytic formula for the diffusion flux. the results that the dispersive particles promote the formation of nodule-like Al2O3 oxides were explained by analysizing some influencing factors such as temperature of oxidation, size. Con tent and distribution of the dispersive particles. In the meantime. the mechanism that the dispersive particles promote the nucleation and re-formation of protective Al2O3 scale was proposed .Correspondent:(MA Xinqing, Institute of Corresion and Prolection of Metals. Chines Academy of Sciences. Shcnyang 110015)
Key words:  dispersive oxide      CeO_2      α-Al_2O_3 scale      initial stage oxidation     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I21/399

1HindamH,WhittleDP.OxidMet、1982:18:2452whittleDP.StringerJPhilosTransRSocLond,1980:A295:3093WagnerC.CorroSci,1965:5,7514StringerJ,WilcoxBA,JaffeeRI.OxidMet1972;5:115KvernesIA.OxidMet1973:6,456FlowerHM.WilcoxBA.CorroSci,1977:12,2437MoulinP,HuntzAM,BerangerG,LacombeP.SerMetall.1977:11:5338李铁藩,马信清,金属学报,1991;21:B259NagaiH.JJapanInstMet,1981;22:10110HouPY.StringerJJElectrochemSoc,1987:134,193611WahlG.ThinSolidFilms,1983:107:41712WangG,GleesonB,DouglassDL.Oxidmet.199135:33313WallworkGR,HedAZ.oxidmet,1971;3:17114郭大钧,大学数学手册.济南:山东科学出版社,1985:174
[1] WU Yigui;LI Yan;YU Zhonghan;LIU Jiajun;WANG Yu Louyang Institute of Technology Tsinghua University; Beijing Laboratory of Materials;Luoyang Institute of Technology;Luoyang 471039. EFFECT OF CeO_2 ON MICROSTRUCTURE AND WEAR RESISTANCE OF LASER REMELTING FeBSi COATING[J]. 金属学报, 1993, 29(3): 76-79.
No Suggested Reading articles found!