THERMODYNAMICS OF Fe-Mn-C-P MELTS CONTAINING HIGH Mn
GUO Shangxing; DONG Yuanchi(East China Institute of Metallurgy; Ma'anshan 243002)
Cite this article: 

GUO Shangxing; DONG Yuanchi(East China Institute of Metallurgy; Ma'anshan 243002). THERMODYNAMICS OF Fe-Mn-C-P MELTS CONTAINING HIGH Mn. Acta Metall Sin, 1995, 31(18): 241-246.

Download:  PDF(377KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solubility of carbon in Fe-Mn-C-P melts containing high manganese Was determined at 1400℃.The solubility data can be expressed as: N_C=0.1961+0.1183N_(Mn)- 0.8525 Np The interaction coefficients between Mn and C,P and C in this melt were obtained as follows: ε_C ~(Mn)=-1.67,ρ_C ~(Mn)=0.29,ε_C ~P=11.00,ρ_C ~P=10.82 The activity coefficients of Mn,P and Solvent Fe in melts containing high Mn were estimated.
Key words:  Fe-Mn-C-P system      melt manganese      activity coefficient      interaction coefficient     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I18/241

1DarkenLSTransMetallSocAIME,1967:239:902DreslerW.CanMetallQ,1989;28:1093冀春霖,张淼,俞荣祥.东化江学院学报,1987;8:2654 倪瑞明,马中庭,魏寿昆,钢铁研究学报,1990;4:175 EdstromJO,刘晓亚.见:中国一瑞典冶金科技合作第三阶段共同研究论文集,北京:冶金工业出版社,1992:2M6 TurkdoganET,LeakeLE.JIronSteelInst,1955;179:397LupisCHP.ActaMetall,1968;16:13658DurrerG.MetallurqiedesEisens,TheoriederStahlerzeugungI.Berlin:Springer-Verlag,1978:2749ElliottJF,ElectrFurnConfProc,1974;32:6210BodsworthC,BellH.PhysicalChemistryofIronandSteellManufacture,London:Longman,1972:50911PeltonAD,BaleCW.MetallTrans,1986;17A:121112SrikanthS,JacobKT.MetallTrans,1988;19B:26913VenoS,WasedceY,JacobKT,TamakiS.SteelRes,1988;59:474
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
[3] CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25). STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS[J]. 金属学报, 1997, 33(8): 831-837.
[4] XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing. DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn[J]. 金属学报, 1993, 29(1): 65-68.
[5] JIANG Guochang;ZHANG Xiaobing;XU Kuangdi Shanghai University of Technology Correspondent Department of Metallargy and Materials Engineering; Shanghai University of Technology; Shanghai 200072. EVALUATION OF COMPONENT ACTIVITY IN C-Fe-X(X=Si; Mn, Cr, Ni) MELTS[J]. 金属学报, 1992, 28(6): 52-58.
[6] KONG Fanya;YANG Kenu;LU Yong'an;SUN Shuxue Institute of Metal Research; Academia Sinica; Shenyang. CONCENTRATION DISTRIBUTION OF ALLOYINGELEMENT IN SURFACE LAYER OF Ti ALLOY MELTS[J]. 金属学报, 1991, 27(5): 141-143.
[7] NI Ruiming;MA Zhongting;WEI Shoukun University of Science and Technology Beijing associate professor;Faculty of Physical Chemstry of Metallurgy;University of Science and Technology Beijing; Beijing 100083. THERMODYMICS OF Mn-C-j MELTS AT 1350℃[J]. 金属学报, 1990, 26(2): 93-97.
[8] CHANG Heming;DU Ting;YU Jingsheng Central Iron and Steel Research Institute; Beijing. THERMODYNAMIC PROPERTIES OF Fe-V-Ce LIQUID SOLUTION[J]. 金属学报, 1989, 25(2): 152-154.
[9] ZHANG Qianxian University of science and Technology Beijing. DETERMINATION OF ACTIVITY OF Al IN SOLID Cu-Al ALLOYS[J]. 金属学报, 1989, 25(2): 149-151.
[10] NI Ruiming;CHENG Wu;WEI Shoukun Beijing University of Science and Technology Manuscript received 9 March; 1988. SOLUBILITY OF Ca IN Mn AND INTERACTION COEFFICIENTS OF Al AND Fe ON Ca IN Mn AT 1350℃[J]. 金属学报, 1989, 25(1): 81-85.
[11] JI Chunlin;YU Rongxiang Northeast University of Technology;LIU Sulan Leeturer;Department of Metallurgtcal Physicat Chemistry;Northeast University of Technotogy;Shenyang. THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅱ. ACTIVITY OF B AND ITS INTERACTION COEFFICIENTS[J]. 金属学报, 1988, 24(2): 161-165.
[12] JI Chunlin;YU Rongxiang;LIU Sulan Northeast University of Technology; ShenyangLIU Sulan Lecturer;Department of Metallurgleal Phusicat Chemistry;Northeoss University of Technology;Shenyang. THERMODYNAMICS OF TERNARY Fe-B-Si MELTS AT 1450℃ Ⅰ. ACTIVITY OF Si AND ITS INTERACTION COEFFICIENTS[J]. 金属学报, 1988, 24(2): 155-160.
[13] WANG Pengfei;HAN Qiyong Beijing University of Iron and Steel Technology. Ca-O EQUILIBRIA IN LIQUID Fe AND Fe-C ALLOYS[J]. 金属学报, 1988, 24(1): 77-81.
No Suggested Reading articles found!