| IN SITU SEM OBSERVATION ON MICROFRACTURE OF TA2/A3 EXPLOSION CLADDING INTERFACE |
| YANG Yang;ZHANG Xinming(Central-South University of Technology; Changsha); LI Zhenghua; LI Qingyun(North-West Institute for Nonferrous Metal Research; Baoji)(Manuscript received 13 December;1993) |
|
Cite this article:
YANG Yang;ZHANG Xinming(Central-South University of Technology; Changsha); LI Zhenghua; LI Qingyun(North-West Institute for Nonferrous Metal Research; Baoji)(Manuscript received 13 December;1993). IN SITU SEM OBSERVATION ON MICROFRACTURE OF TA2/A3 EXPLOSION CLADDING INTERFACE. Acta Metall Sin, 1994, 30(9): 409-415.
|
|
|
Abstract In-situ SEM observations on TA2/A3 explosion cladding interfaces have been performed to examine the microfracture behaviour. The microfracture mechanism of explosion cladding TA2/A3 interface seems that the microcracks initiate inside the swirls or inside the molten material as well as at the boundary between the molten material and the A3 matrix,and penetrate into the nearby A3 matrix in the direction normal to the tensile load direction under the action of the crack-tip stress field. At the same time, the microcracks initiate along the TA2 /A3 interface, and link up under the tensile load. Terminal cleavage fracture takes place mainly in the recrystallized and grain abnormal growth region on the A3 side in the vicinity of TA2/A3 interface.Localized fracture takes place along the interface molten layer.Correspondent: YANG Yang.(Departnient of Materials. Central-South University of Technology.Changsha 410083)
|
|
Received: 18 September 1994
|
| 1段文森,鲁汉民,吴敬梓.稀有金属材料与工程,1989;3:62鲁汉民,段文森,吴敬梓.稀有金属材料与工程,1989;2:193YoshiiK,KawobeH,YamadaT.MechBehavMater.1972;1:25764HorsthPJ,WilsonRN.JInstMet,1963;92:825TetelmanAS,RobertsonWD.ActaMetall,1963;11:4156StrohAN.procRSocLondon,1954;223A:4041955;232A:5487CottrellAH.TransAIME,1958;212:1928WeissBZ.ZMetallk,1971;62:1590 |
| No Suggested Reading articles found! |
|
|