| EFFECTS OF ELECTROMAGNETIC FLUID FLOW ON Al-Al_2Cu EUTECTIC MORPHOLOGIES |
| JIAO Yuning;LIU Qingmin;YANG Yuangsheng;GE Yunlong;HU Zhuangqi(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 4 October;1993;in revised form 12 November;1993) |
|
Cite this article:
JIAO Yuning;LIU Qingmin;YANG Yuangsheng;GE Yunlong;HU Zhuangqi(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 4 October;1993;in revised form 12 November;1993). EFFECTS OF ELECTROMAGNETIC FLUID FLOW ON Al-Al_2Cu EUTECTIC MORPHOLOGIES. Acta Metall Sin, 1994, 30(6): 286-288.
|
|
|
Abstract The solidification behaviour of Al-33% Cu eutectic alloy under the influnence of an electromagnetic fluid flow has been studied.It is found that with the increase of flow velocity,the Al-Al2Cu eutectic morphologies changes from regular laminae to unregular laminae,unregular rods up to regular rods and the laminar spacingsλ have a little increase.The solute redistribution caused by fluid flow is a main factor for the formation of unregular and other eutectic morphologies.
|
|
Received: 18 June 1994
|
| 1VerhoevenJD,HomerRH.MetallTrans,1970;12:34372MollardFR,FlemingsMC.TransTMS-AIME,1967;239:15343TillerWA.TransAFS,1979:209` |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|