SLIP SYSTEMS AND THEIR CHARACTERISTICS OF Nb SINGLE CRYSTALS UNDER TENSION, COMPRESSION AND CYCLIC DEFORMATION
WU Jiansheng; LIN Dongliang(Shanghai Jiao Tong University)(Manuscript received 11 October;1993; in revised form 20 December; 1993)
Cite this article: 

WU Jiansheng; LIN Dongliang(Shanghai Jiao Tong University)(Manuscript received 11 October;1993; in revised form 20 December; 1993). SLIP SYSTEMS AND THEIR CHARACTERISTICS OF Nb SINGLE CRYSTALS UNDER TENSION, COMPRESSION AND CYCLIC DEFORMATION. Acta Metall Sin, 1994, 30(5): 187-194.

Download:  PDF(565KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The slip systems of Nb single crystals with single and multiple glide orientations have been investigated respectively under tension, compression and cyclic defomation. From the stereographic plots of the slip line directions measured around the specimen surface,the slip planes were determined. The slip system for the single glide orientation ([321] orientation) is(101) under tension, however in compression, it is(101) and (213) . The relationship of the slip systems activated by tensile,compressional and cyclic deforination was analyzed in accordance with the deformation features of bcc crystals. The surface topography of the specimens has been observed using optical microscope, SEM and TEM(replical).The activated sequence of the slip systems for the multiple slide orientation ([110] orientation) was therefore determined. Correspondent: WU Jiansheng, professor, Department of Malerials Science, Shanghai Jiao Tong University, Shanghai 200030
Key words:  Nb single crystals      slip system      activated sequence     
Received:  18 May 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I5/187

1DuesbeyMS,FoxallRA,HirschPB.JPhys(Paris),1966;27(Suppl.7-8):C3-1932TaylorG,ChristianJW.PhilosMag,1967;15:8733AngladaM,GuiuF.PhilosMagA,1981;44:4994SiederslebenME,TaylorG.PhilosMagA,1989;60:6315林栋梁,吴建生,陈贤芬.金属学报,1989;25:A1216林栋梁,吴建生.金属学报,1988;24:A767胡赓祥,钱苗根.金属学.上海:上海科学技术出版社,1980:2728田莳,李秀臣,李邦淑.金属物理性能.北京:国防工业出版社,1985:154
[1] Shoudong CHEN,Xianghua LIU,Lizhong LIU,Meng SONG. CRYSTAL PLASTICITY FINITE ELEMENT SIMULA- TION OF SLIP AND DEFORMATION IN ULTRA- THIN COPPER STRIP ROLLING[J]. 金属学报, 2016, 52(1): 120-128.
[2] LIU Jiangtao;WANG Zhongguang;SHANG Jianku. DEFORMATION BEHAVIORS OF [110] AND [112] ORIENTED β-Sn SINGLE CRYSTALS[J]. 金属学报, 2008, 44(12): 1409-1414.
[3] SU Jilong; HU Gengkai. MICROMECHANICAL STUDY ON YIELD STRESS AND THE EFFECTS OF TWINNING FOR γ-TiAl-BASED PST CRYSTALS[J]. 金属学报, 2005, 41(12): 1243-1248 .
[4] SUN Fusheng;GAO Wen;CAO Chunxiao(Institute of Aeronautical Materials; Beijing)(Manuscript received 31 August; 1993; in revised form 22 November; 1993). INFLUENCE OF DEFORMATION TEMPERATURE ON α_2-PHASE SLIP SYSTEMS OF A Ti_3Al ALLOY[J]. 金属学报, 1994, 30(11): 507-514.
[5] NING Hua;ZHANG Lixin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. METALLOGRAPHIC STUDY ON SEGREGATION BEHAVIOUR OF P IN COLD ROLLED Fe-P ALLOYS DURING ANNEALING[J]. 金属学报, 1990, 26(5): 34-38.
No Suggested Reading articles found!