| REDUCTION OF CaO-SiO_2-Al_2O_3-Fe_ tO QUARTERNARY SLAG SYSTEM BY CO |
| YANG Xuemin; GUO Zhancheng; YU Xianpu; AI Jing; WANG Daguang (Institute of Chemical Metallurgy; Chinese Academy of Sciences; Beijing)(Manuscript received 25 March;1994) |
|
Cite this article:
YANG Xuemin; GUO Zhancheng; YU Xianpu; AI Jing; WANG Daguang (Institute of Chemical Metallurgy; Chinese Academy of Sciences; Beijing)(Manuscript received 25 March;1994). REDUCTION OF CaO-SiO_2-Al_2O_3-Fe_ tO QUARTERNARY SLAG SYSTEM BY CO. Acta Metall Sin, 1994, 30(23): 491-498.
|
|
|
Abstract The reduction of CaO-SiO_2-Al_2O_3-Fe_tO quarternary slag system by CO has been investigated. Apparent reduction rate constant K_ a was determined by mesuring CO_2 evolution from reaction tube with an infrared gas analyser. Adding Al_2O_3 to CaO-SiO_2-Fe_tO ternary slag increases both K_a and reduction rate constant K of CaO-SiO_2-Fe_tO ternary slag. K_a increases and K changes parabolicly with increasing Fe_tO content for CaO-SiO_2-Al_2O_3-Fe_tO slag system at constant slag basicity (B=CaO/SiO_2),and K approaches to the minimum when Fe_tO content is about 60%. K_a increases linearly and K takes a decrease tendency with the increase of optical basicity for A_(FeO) chosen as 1.0 or 0.87. The equation of calculating a_(Fe_tO) for CaO-SiO_2-Al_2O_3-Fe_tO slag system has been derived based on regular solution model and calculated a_(Fe_tO) values are in fairly agreement with bibliography reported data except for extremely Fe_tO rich region.(Correspondent: YANG Xuemin, Institute of Chemical Metallurgy, Chinese Academy of Sciences, Beijing 100080)
|
|
|
| 1NagaskaT,IguchiY,Ban-yaS.FifthInternationalIronandSteelCong.April6-9,l986,WashingtonDC,USA,6692FineH,MeyerD,JankeD,EngelH-J.IronmakingSteelmaking,1985,12(4):1573杨学民,王大光,宣德茂,唐武成,第八届冶金物理化学学术研讨会论文集,苏州,1992:1534杨学民,王大光,刘天中,宣德茂,唐武成.化工冶金,1994:15:75杨学民,王大光,宣德茂,唐武成.化工冶金,1993;14:1956杨学民,王大光,宣德茂,唐武成,化工冶金,1995;16:77杨学民,王大光,宣德茂.金属学报,1993;29:B3418DuffyJA,IngramMD.JAmChemSoc.,1991;93:64489YoungRW,DuffyJA,HassallGJ,XuZ..IronmakingSteelmakig,1992;19:20110BergmanA.SteelRes,1990;61:34711GaskellDR.TransISIJ,1982;22:99712NagabayashiR,HinoM,Ban-yaS.ISIJInt,1989;29:14013Ban-yaS.ISIJInt,1993;33:214万谷志郎,日野光兀,汤下宪志,铁钢,1985;71:85315万谷志郎,日野光兀,竹添英孝.铁钢,1985;71:190316Ban-yaS,HinoM.ChemicalPropertiesofMoltenSlags.Tokyo:TheIronandSteelInstituteofJapan,1991:275 |
| No Suggested Reading articles found! |
|
|