| EFFECTS OF HYDROGEN ATOMS OF INITIATION AND PROPAGATION OF CRACKS UNDER SLOW LOADING |
| HAN Guangwei(Central Iron and Steel Research institute Ministry of Metallurgical Industry); SONG Yujiu; (Xi′an Jiaotong University)(Manuscript received 9 November; 1993; in revised form 3 June; 1994) |
|
Cite this article:
HAN Guangwei(Central Iron and Steel Research institute Ministry of Metallurgical Industry); SONG Yujiu; (Xi′an Jiaotong University)(Manuscript received 9 November; 1993; in revised form 3 June; 1994). EFFECTS OF HYDROGEN ATOMS OF INITIATION AND PROPAGATION OF CRACKS UNDER SLOW LOADING. Acta Metall Sin, 1994, 30(10): 448-452.
|
|
|
Abstract The effects of hydrogen atoms on crack initiation and propagation have been studied in normalized Cr-1Mo steel using in situ SEM tensile experiment. The results are found that the critical plastic deformation at notch root for initiation of ductile crack is reduced by charging hydrogen, and the crack propagation pattern is also changed from continuous growth on the plane of maximum shear stress to uncontinuous growth on maximum normal stress plane. Hydrogen induced plastic deformation has not been found, and the effect mechanisms of hydrogen atoms are analysized.Correspondent: HAN Guangwei, Department 5, Central Iron and Steel Research Institute, Ministry of Metallurgical Industry, Beijing 100081
|
|
Received: 18 October 1994
|
| 1DoigP,JonesGT.MetallTrans,1977;8A:19932McMahonCJ,VitekV,JoklML.Fracture′77,NewYork:PergamonPress,3633ThompsonAWMetallTrans,1979;10A:7274韩光炜.西安交通大学博士学位论文,19925孙军.西安交通大学博士学位论文,1989 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|