| CRYSTALLOGRAPGY OF LATH MARTENSITE IN ULTRAHIGH-STRENGTH STEEL 300M |
| LUO Chengping;XU Linkang;CHA Jianzhong South-China University of Technology; Guangzhou Guangdong Iron and Steel Research InstituteDepartment of Mechanical Engineering(Ⅱ);South-China University of Technology; Guangzhou 510641 |
|
Cite this article:
LUO Chengping;XU Linkang;CHA Jianzhong South-China University of Technology; Guangzhou Guangdong Iron and Steel Research InstituteDepartment of Mechanical Engineering(Ⅱ);South-China University of Technology; Guangzhou 510641. CRYSTALLOGRAPGY OF LATH MARTENSITE IN ULTRAHIGH-STRENGTH STEEL 300M. Acta Metall Sin, 1993, 29(7): 28-33.
|
|
|
Abstract A TEM study was made of the crystallography of the lath martensite formedin a Ultrahigh-strength steel 300M. It was found that the habit plane is close to {335}_A, theorientation relationship between the martensite and austenite is the G-T one which is 2.5°away from the K-S relationship, and the laths relate to each other by a relative rotation ofabout 60° about the normal to their common planes {110}_M. Although various orientationrelationships, including a near {112}_M twin one, could be formed between the lathsthemselves due to the rotations, a unique G-T orientation relationship was kept between thelath and austenite.
|
|
Received: 18 July 1993
|
1 牧正志,田村今南,铁钢,1981;67:852. 2 Rao Narasimha B V, Metall Trans, 1979; 10A: 645. 3 Rao Narasimha B V, Thomas G, Proc. of 3rd Int Conf on Martensitic Transformations, Boston, 1979; P12. 4 Sarikaya M, Thomas G, Journal De Physique, 1983; 43: C4--563. 5 Horn R M, Ritchie R O, Metall Trans, 1978; 9A: 1039. 6 Luo C P, Weatherly G C, Acta Metall, 1987; 35: 1963. 7 Luo C P, Weatherly G C, Liu Z Y, Metall Trans, 1992; 23A: 1403. |