| APPLICATION OF d-ELECTRON ALLOY DESIGN THEORY TO DEVELOPMENT OF HOT CORROSION RESISTANT Ni-BASE SINGLE CRYSTAL SUPERALLOYS——Ⅱ. Effects of Refractory Metals Ti, Ta and Nb on Microstructure and Properties |
| ZHANG Jishan;CUI Hua;HU Zhuangqi;MURATA Y;MORINAGA M;YUKAWA N Institute of Metal Research; Academia Sinica; Shenyang Toyohashi University of Technology; Japanassociate professor;Institute of Metal Research;Academia Sinica;Shenyang 110015 |
|
Cite this article:
ZHANG Jishan;CUI Hua;HU Zhuangqi;MURATA Y;MORINAGA M;YUKAWA N Institute of Metal Research; Academia Sinica; Shenyang Toyohashi University of Technology; Japanassociate professor;Institute of Metal Research;Academia Sinica;Shenyang 110015. APPLICATION OF d-ELECTRON ALLOY DESIGN THEORY TO DEVELOPMENT OF HOT CORROSION RESISTANT Ni-BASE SINGLE CRYSTAL SUPERALLOYS——Ⅱ. Effects of Refractory Metals Ti, Ta and Nb on Microstructure and Properties. Acta Metall Sin, 1993, 29(7): 13-22.
|
|
|
Abstract A study was conducted of the effects of refractory metals Ti, Ta and Nb on themicrostructures and properties of a hot corrosion resistant alloy system Ni-16Cr-9Al- 4Co-2W-1Mo-(0-4)Ti-(0-4)Nb, in at.-%, which was selected based on the d-elec-trons alloy design theory and some basic considerations of an alloying features of single crys-tal Ni-base superalloys. The contour lines of solidification reaction temperatures and eutectic(γ+γ′) volume fraction in the Ti-Ta-Nb compositional triangle were determined by DTA andimaging analyzer. Compared with the reference alloy IN738LC, in most of the compositionalranges studied, the designed alloys show very low amount of eutectic (γ+γ′), ≤0.4 v.-%, low-er solidification range, ≤65℃, and wider "heat treatment window", >100℃, which indi-cates that the alloys should have the promising microstructural stability, single crystalcastability and be easier for complete solution treatment. In wide compositional ranges, thedesigned alloys showed good hot corrosion resistance (mass loss less than 20 mg / cm~2 after24 h kept in moiten salt at 900℃). By summarizing the results, the promising alloy,compositional ranges with balanced propertise were determined for the final alloy design step,i.e., the single crystal growth and mechanical property characterization of the alloys selectedfrom the above regions.
|
|
Received: 18 July 1993
|
1 张济山,崔华,胡壮麒,村田纯教,森永正彦,汤川爱夫,金属学报,1993:29;A289 2 Stoloff N S, The Superalloys, ed. Sims C T, Hagel W C, A Wiley-Interscience Publication, (1972) 79. 3 Nathal N V, Ebert L J, Metall Trans, 1985; 16A: 1984 4 Matsugi K, Yokoyama R, Kawamura Y, Ishihara H, Murata Y, Morinaga M, Yukawa N, Report of the 23rd Committee on Heat-Resisting Metals and Alloys, Japan Society for the Promotion of Science, 1985; 16A: 1984 5 Hull P C, Met Prog, 1969; 96: 139 6 Decker R F, Sims C T, The Superalloys, ed, Sims C T, Hagel W C, A Wiley-Interscience Publication, (1972) 33. 7 张济山,崔华,胡壮麒,村田纯教,森永正彦,汤川爱夫,金属学报,1993. 8 Yukawa N, Morinaga M, Murata Y, Ezaki Hand Inoue S, Superalloys 1988, ed. D. N. Duhl, et al., AIME, (1988) 225. 9 Matsugi K, Yokoyama R, Murata Y, Morinaga M, Yukawa N, Proc of Inter Conf on High Temperature Materials for Power Engineering 1990, ed, E. Backelet et al., C. R. W., (1990) 1251. 10 Zhu Y S, Zhang S N, Xu L Y, Bi J, Hu Z Q, Shi C X, Superalloys 1988, ed, Dubl D N et al., AIME, (1988) 703. 11 Janovski G M, Heckel R W, Pletka B J, Metall Trans 1986; 17A: 1891w |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|