Abstract With the aid of 3-dimensional topological analysis methodology, relation-ships among phase regions on the isotherm section of the Nd-Fe-B phase diagram at 1000℃and those on vertical sections of the Pr-Fe-B phase diagram passing through Pr_2Fe_14B pointhave been re-discussed and modified.
|
Received: 18 March 1993
|
1 Hillert M. Int: Metals Rev, 1985: 30 (2) : 45 2 Rhines F N. Phase Diagrams in Metallurgy. New York: McGraw-Hill, 1956; 204 3 Matsuura Y, Hirosawa S, Yamamoto H, Fujimura S, Sagawa M, Osamura K. Jpn J Appl Phys. 1985; 24: L635 4 张宁,罗阳,金属学报.1989;25:B104 5 张宁,罗阳,金属学报.1989;25:B109 6 车广灿,梁敬魁,王选章,中国科学.1985;A(10) :909 7 Schneider G, Henig E-T, Petzow G, Stadelmaier H H. Z Metallkde, 1986; 77: 755 8 Henig E-T. Schneider G. Stadelmaier H H. Z Metallkde, 1987: 78 (11) : 818 9 Zhang W, Liu G, Han K. In: Massalski et al. eds., Binary Alloy Phase Diagrams. 2nd ed. ASM International, 1990; 1732 1O 徐平国,北京科技大学硕士学位论文,1991;79 11 Hao S. Xu W. J Chin Rare Earth Soc. 1990; 8 (3) : 200 12 田静华,黄毅英,梁敬魁,中国科学.1987;A(2) :159S |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|