| SUPERPLASTIC WELDING OF STEELS 40Cr-CrWMn |
| WEN Jiuba;XI Jukui Luoyang Institute of Technology |
|
Cite this article:
WEN Jiuba;XI Jukui Luoyang Institute of Technology. SUPERPLASTIC WELDING OF STEELS 40Cr-CrWMn. Acta Metall Sin, 1993, 29(10): 92-96.
|
|
|
Abstract Superplastic welding of steels 40Cr-CrWMn, with prior surface treatment oforganic solution protecting coating after thermo-mechanical treating, may be performed inair in a furance under conditions: temperature ranged 750--780℃, strain rate 2×10~(-4) s~(-1),pressure 50--90 MPa, and time 3--5 min. The welds seem to have similar strength to the basesteel 40Cr. The microstructure of welds was analyzed under SEM and TEM. Themicromechanism for superplastic welding of steels was suggested as the disappearance of orig-inal bond interfaces caused by atomic diffusion and grain sliding during superplasticdeformation.
|
|
Received: 18 October 1993
|
1 Oshita T, Takei H, Hatayama T. J Jpn Inst.Met, 1985;49:552 2 Collins J F, Highberger W T. Met Prog, 1981; 119:79 3 黄岩,马龙翔.金属学报,1992;28:B413 4 文九巴,席聚奎,杨蕴林.材料科学进展,1992;6(2) :133 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|