Abstract The damage behaviour of Fe-Cr-Mn alloys during electron irradiation isshown to be different from that in Fe-Cr-Ni alloy. The difference appears to be a conse-quence of the different diffusion behaviour of Ni and Mn due to interaction between soluteatoms and point defects. Especially the interaction between Mn atoms and vacancies inFe-Cr-Mn is strong so that the migration energy becomes greater than that in Fe-Cr-Ni al-
|
|
Received: 18 October 1993
|
1 Brager H R, Garner F A, Gelles D S, Hamilton M L. J Nucl Mater, 1985; 133--134: 907 2 Takahashi H, Takeyama T, Tanikawa K, Miura R. J Nucl Mater. 1985; 133--134: 566 3 Takahashi H, Ohnuki S, Kinoshita H, Nakahigashis. J Nucl Mater, 1991; 179--181: 629 4 桐谷道雄.金属学会会志,1967;8:553 5 Watanabe H, Aoki A, Murakami H, Yoshida N. J Jpn Inst Met, 1988; 152: 536 6 Kiritani M, Yoshida N, Takata H, Machara Y. J phy Soc Jpn, 1975; 138: 1677 7 Kiritani M, Takata H, Moriyama K, Eiich Jujita F. Phylos Mag 1979: A40: 779 8 Rehn L E, Okamoto P R, Potter D L, Wiedersich H. J Nucl Mater, 1978; 74: 242 9 Deschepper L, Cornells J, Knuyt G, Nihoul J, Stals L. Phys status solidi, 1980; (a) 61: 3 10 Tabata T, Fujita H, Igaki K, Isshiki M, Scr Met, 1981; 14: 1317 11 胡本芙,高桥平六郎,竹山太郎,金属学报,1990;26:1V |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|