CALCULATION OF BAINIT TRANSFORMATION KINETICS IN Fe-C-Si-Mn ALLOYS
YANG Liu;LIU Shikai;YANG Ping Southwest Jiaotong University; Chengdu
Cite this article: 

YANG Liu;LIU Shikai;YANG Ping Southwest Jiaotong University; Chengdu. CALCULATION OF BAINIT TRANSFORMATION KINETICS IN Fe-C-Si-Mn ALLOYS. Acta Metall Sin, 1993, 29(1): 1-5.

Download:  PDF(395KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Both regular solution and supper-component models were used to calculatethe driving force for isothermal transformation of Fe-C-Si-Mn alloys. The relativenucleation rate and incubation period were estimated based on the calculated driving force.The results suggest that for carbon-free alloys, the incubation is principally determined by thedriving force, while for carbon-contained alloys, the driving force is not the dominant factor.The result is considered to be in accordance with what is prodicted by the solute drag-like ef-fect (SDLE) theory on the transformation kinetics.
Key words:  transformation kinetics      driving force      Fe-C-Si-Mn alloy     
Received:  18 January 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I1/1

1 刘世楷,杨柳,张筠,朱德贵.金属学报,1992;28:A510
2 杨柳,方鸿生,陈南平.金属学报.1989;25:A264
3 Aaronson H I, Domian H A, Pound G M. Trans AIME, 1966; 236: 768
4 Bhadoshia H K D H. Met Sci. 1981, l5: 178
5 杨柳,方鸿生,孟至和.金属学报,1992;28:A16
6 Lange W F Ⅲ, Enomoto M, Aaronson H I. Metall Trans. 1988, 19A: 427
7 杨萍,西南交通大学硕士学位论文,1991
8 Purdy G R. In: Aaronson H I ed., Proc Int Con f Solid-Solid Phase Transformation, Warrendale, PA, AIME, 1981: 543
9 Aaronson H I. The Mechanism of Phase Transformation in Crystalline Solids. London: Institute of Metals, 1969: 270
[1] Shixin XU, Wei YU, Shujia LI, Kun WANG, Qisong SUN. Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure[J]. 金属学报, 2018, 54(8): 1113-1121.
[2] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. CALCULATION OF TRANSFORMATION DRIVING FORCE FOR THE PRECIPITATION OF NANO-SCALED CEMENTITES IN THE HYPOEUTECTOID STEELS THROUGH ULTRA FAST COOLING[J]. 金属学报, 2013, 49(1): 26-34.
[3] Na Wang; Zhenmin Du. Driving Force for the Nucleation from Supercooled Liquid and Thermodynamic Analysis of Glass Forming Ability for Binary Alloys[J]. 金属学报, 2008, 44(9): 1111-1115 .
[4] XIONG Ying. A TWO-PARAMETER DRIVING FORCE FOR FATIGUE CRACK GROWTH[J]. 金属学报, 2008, 44(11): 1348-1353 .
[5] 许良红 Xu Liang-Hong; tian zhiling Tian. The investigation of the oriented precipitate-free zone in high strength aluminum alloy welds[J]. 金属学报, 2008, 44(1): 91-97 .
[6] ZHANG Wangfeng; ZHU Jinhua; CAO Chunxiao. A New Model on the Law of Mixture Strength for Metastable Materials[J]. 金属学报, 2005, 41(1): 89-.
[7] XU Zuyao T. Y. Hsu. Effect of Stress on Bainitic Transformation in Steel[J]. 金属学报, 2004, 40(2): 113-119 .
[8] TIAN Sugui ; ZHOU Huihua ; ZHANG Jinghua; YANG Hongcai ; XU Yongbo;HU Zhuangqi ( State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)( Department of Materials Science and Engineering; Northeastern University ; Shenyang 110006)( Department of Materials Science and Engineering; Shenyang Polytechnic University; Shenyang 110023)Correspondent: TIAN Sugui; associate professor Tel: (024)5927399. A DIRECTIONAL COARSENING MECHANISM OF THE γ'-PHASE DURING CREEP OF A SINGLE CRYSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(6): 591-596.
[9] (TIAN Sugui ; ZHOU Huihua; ZHANG Jinghua;YANG Hongcai;XU YOngboHU Zhuangqi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal ReSearch; The Chinese Academyof Sciences; Shenyang 110015)(Department of Materials Sciences and Engineering; Northeastern University; Shenyang 110006)(Department of Metal Materials Engineering; Shenyang Polytechnic University 110023)Correspondent:TIAN Sugui; associate professor; Tel: (o24)-25927399; Fax: (024)e3891s2oManuscript received 1997-12-23; in revised form 1998-03-16. DIRECTIONAL COARSENING OF THE γ'-PHASE DURING COMPRESSION CREEP OF A SINGLE CRVSTAL NICKEL-BASE SUPERALLOY[J]. 金属学报, 1998, 34(12): 1261-1266.
[10] LIU Zhenyu; WANG Guodong;(Department of Metal Forming; Northeastem University; Shenyang 110006) ZHANG Qiang (State Key Laboratory of RollingTechnology and Tandem Rolling Automation; Northeastern University; Shenyang110006). GRAIN SIZE PREDICTION AFTER CONTINUOUSLY COOLING TRANSFORMATION FROM DEFORMED AUSTENITE TO FERRITE[J]. 金属学报, 1995, 31(22): 468-172.
[11] LI Shuchen;LIU Shikai Southwestern Jiaotong University; Chengdu. MULTICOMPONENT SEGREGATION ALONG BOUNDARY AND THERMODYNAMICAL ANALYSIS OF Fe-C-Si-Mn ALLOY[J]. 金属学报, 1991, 27(3): 101-105.
[12] LI Chao;WANG Jianli;LIU Jinfang Harbin Institute of Technology. INFLUENCE OF PRE-TRANSFORMED MARTENSITE ON KINETICS OF BAINITIC TRANSFORMATION IN GCr15 STEEL[J]. 金属学报, 1991, 27(1): 16-19.
[13] LI Jian;SUN Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. ON THE KINETICS OF DEFORMED AUSTENITE TO PROEUTECTOID FERRITE TRANSFORMATION[J]. 金属学报, 1990, 26(5): 66-69.
[14] SUN Enxi;YANG Dazhi;XU Zuyao;YANG Fumiug;ZHAO Ruwen Dalian Institute of Railway Dalian University of Technology Shanghai Jiaotong University Institute of Physics; Academia Sinica; Beijing professor. PULSED MAGNETIC FIELD-INDUCED MARTENSITIC TRANSFORMATION IN AN Fe-21Ni-4Mn ALLOY[J]. 金属学报, 1990, 26(4): 12-17.
[15] LIN Guangming;HUANG Yuanshi;ZHANG Jinxiu Zhongshan University; Guangzhou LIN Guangming; Associate Professor; Department of Physics; Zhongshan University;Guongzhou 510275. TRANSFORMATION OF TWO WAY SHAPE MEMORY MATERIAL CONSTRAINED BY STRESS[J]. 金属学报, 1989, 25(6): 16-21.
No Suggested Reading articles found!