| ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM |
| LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang) |
|
Cite this article:
LIU Xingjun; HAO Shiming; SUN Rongyao; (Northeast University of Technology; Shenyang). ISOTHERMAL SECTION AT 1000 AND 1100℃ OF Fe-Mn-AI SYSTEM PHASE DIAGRAM. Acta Metall Sin, 1992, 28(7): 50-54.
|
|
|
Abstract Phase equilibria at Fe-Mn side of isothermal section at 1000 and 1100℃ in Fe-Mn-Al system have been determined using the diffusion couple, technique and metallography. A three-phase, α+γ+β, region was found at 1000℃. The method of solid/gas diffusion couple used to determine equilibrium phase composition is believed to be feasible for the system containing volatile component.
|
|
Received: 18 July 1992
|
1 Banerji S. Adv Met Prog, 1987; 4: 59 2 Charles J, Berghezan A, Lutts A, Dancoisne P L. Met Prog, 1981; 119(6) : 71 3 张彦生.金属学报,1986;22:A470 4 Schmatz D J. Trans AIME, 1959; 215: 112 5 Chakrabarti D J. Metall Trans, 1977; 8B: 121 6 郝士明,刘兴军.中国物理学会第五届全国相图会议文集,武汉,1988) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|