| EVALUATION OF COMPONENT ACTIVITY IN C-Fe-X(X=Si; Mn, Cr, Ni) MELTS |
| JIANG Guochang;ZHANG Xiaobing;XU Kuangdi Shanghai University of Technology Correspondent Department of Metallargy and Materials Engineering; Shanghai University of Technology; Shanghai 200072 |
|
Cite this article:
JIANG Guochang;ZHANG Xiaobing;XU Kuangdi Shanghai University of Technology Correspondent Department of Metallargy and Materials Engineering; Shanghai University of Technology; Shanghai 200072. EVALUATION OF COMPONENT ACTIVITY IN C-Fe-X(X=Si; Mn, Cr, Ni) MELTS. Acta Metall Sin, 1992, 28(6): 52-58.
|
|
|
Abstract The parameters in the polynomial expression of partial mole free energy of Cwere evaluated by value fitting method on the basis of boundary conditions of liquid domainon the system C-Fe-X(X=Si, Mn, Cr, Ni). Then the activity coefficient of the element Xmaybe calculated with the I-D method. The approach suggested is proved to be useful for theactiveity evaluation of every element in the whole liquid domain of the concerncd 4C-Fe-Xternary systems. The results are found in a good agreement with those of citedprovious literatures.
|
|
Received: 18 June 1992
|
1 Pelton A D, Flengas S N. Can J chem, 1969; 47: 2283--2293 2 王之昌.中国科学(A),1986;(8) :862-873 3 王之昌.私人通讯 4 Hultgren R et al. Selected Values of Thermodynamic Properties of Metals and Alloys. New York: Wiley. 1973: 485 5 Kubaschewsk O et al., Metallurgical thermochemistry. 5th ed, Oxford: Pergamon, 1979 6 Elliott J F, Gleiser M, Ramakrishna V. Thermochemistry for Steelmaking. Vol. Ⅱ Thermodynamic and Transport Propertties, London: Addison-Wesley, 1963 7 Darken L S. Trans Metall Soc AIME 1967; 239: 90--96 8 Dresler W. ISM, 1990: 95--99 9 Griffing N R, Forgeng W D, Healy G W. Trans Metall Soc AIME, 1962; 224: 148--158 10 Dresler W. Electr Furace Conf Proc, 1989; 47: 49--55 11 Dresler W. Can Metall Q, 1989; 28: 109--115 12 张晓兵.上海工业大学学报,1990;11;490--496 13 Turkdogan E T. Iron Steel Inst Jpn, 1956; 5: 69--72G |