ELECTROCHEMICAL ALLOYING OF Ni IN MOLTEN NaCl-KCl-PrCl_3 |
YANG Qiqin;LIU Guankun;TONG Yexiang;LIANG Guangchao Zhongshan University; Guangzhou |
|
Cite this article:
YANG Qiqin;LIU Guankun;TONG Yexiang;LIANG Guangchao Zhongshan University; Guangzhou. ELECTROCHEMICAL ALLOYING OF Ni IN MOLTEN NaCl-KCl-PrCl_3. Acta Metall Sin, 1992, 28(3): 65-68.
|
Abstract The cyclic vltammetry, electrode potential--time curve after potentiostatic elec-trolysis, potential step method and X--ray diffraction were used to study the electrode process ofPr(III) reduced on Ni electrode in molten NaCl--KCl--PrCl_3 and to determine the diffusioncoefficient of Pr into its alloy phase. The Pr-Ni alloys are formed before the deposition of me-tallic Pr. The PrNi_5 is formed on electrode first and then the intermetallic compounds containedmore Pr are formed in sequence. The standard free energy of formation for PrNi_5 has also beendetermined.
|
Received: 18 March 1992
|
1 Metsumoto T, Matsushita A. J Less-Common Met, 1987; 132(1) : 115 2 Strzeszewski J, Nazareth A, Hadjipanayis G C. J Appl Phys, 1988; 63: 3978 3 中村永治,井户胜寿.日本公开特许,62 222 092,1987 4 Flengas S N, Ingraham T R. J Electrochem Soc, 1959; 106: 714 5 Hamer W J, Malmberg M S, Rubin B. J Electrochem Soc, 1956; 103: 8 6 Kabanov B N, Astakhov I I, Kiseleva I G. Electrochim Acta, 1979; 24: 167 7 Bard A J, Faulkner L R. Electrochemical Methods. New York: John Wiley & Sons, 1980 8 Mamantov G, Manning D L, Dale J M. J Electroanal Chem, 1965; 9: 253 9 章复中,谷力军,稀土,1982;(1) :56 10 杨绮琴,刘冠昆,蔡伟文,刘泽锦.稀有金属,待发表 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|