Export:  BibTeX | EndNote (RIS)      
Abstract  Pattern recognition method is used for the investigation of stability region of filled Ti_2Ni phases in multi-dimensional bond-parameter space: The filling of C, N and O atoms into T_6 octahedra consisting of atoms of early-transition elements makes the expansion of the stability region of Ti_2Ni phase, and the relative stability of Al_2Cu and MoSi_2 type compounds decreases after the introduction of non-metallic elements such as C, N and O.
Key words:  filled Ti_2Ni phase      stability region      pattern recognition     
Received:  18 November 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I11/20

1 Chen Nianyi, Xie Leiming, Shi Tiansheng, Jiang Naixiong, Li Qingzhi. Scientia Sinica, 1981; 24: 1528
2 周班,金石鸣,邵俊,陈念贻.金属学报,1989;25:B203
3 Giessen B G. Developments in the Structure Chemistry of Alloy Phase. New York: Plenum Press, 1969: 153
4 Massalski T B. Binary Alloy Phase Diagrams. Metals Park, Ohio: ASM, 1989~
[1] ZHANG Xiaoqing; SUN Yongqing; ZHANG Zheng. Recognition of Metal Fracture Surface Morphologies Based on the Fuzzy Texture Spectrum[J]. 金属学报, 2004, 40(10): 1018-1022 .
[2] ZHANG Zhaochun; WU Zhu; LI Chonghe; QIN Pei; CHEN Nianyi(Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)Correspondent: WU Zhu; Tel: (021)62511070-8932; Fax: (021)62513510. APPLICATION OF PATTERN RECOGNITION AND ARTIFICIAL NEURAL NETWORK TO IMPROVE THE MECHANICAL PROPERTIES OF CYLINDER BLOCK CAST OF AUTOMOBILE ENGINE[J]. 金属学报, 1998, 34(10): 1068-1072.
[3] CONG Peisheng; LI Tonghua (Tongji University; Shanghai) CHEN Yu; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica; Shanghai). NEURON ADAPTIVE ALGORITHM APPLIED TO EXPERIMENTAL DESIGN IN STEEL PRODUCTION[J]. 金属学报, 1992, 28(11): 59-61.
[4] CHEN Yu; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica)PENG Ping; KONG Bingyu (Iron and Steel Research Institute; Shanghai Baoshan Iron and Steel Complex). ASPRES—AN EXPERT SYSTEM FOR ALLOY STEEL DEVELOPMENT[J]. 金属学报, 1992, 28(10): 91-94.
[5] LIU Miaoxiu;CHENG Zhaonian;CHEN Nianyi;KE Jiajun Shanghai Institute of Metallurgy; Academia Sinica Institute of Chemical Metallurgy; Academia Sinica; Beijing. FACTORS AFFECTING SILICA CONTENT OF ALUMINIUM HYDROXIDE PRODUCT IN CARBONIZATION PROCESS[J]. 金属学报, 1990, 26(5): 156-159.
No Suggested Reading articles found!