STABILIZATION OF MARTENSITE AND PARENT PHASE ORDERING IN A Cu-Zn-Al ALLOY
CHEN Shuchuan;XU Zuyao T. Y. Hsu; YANG Fan Shanghai Jiaotong University; ZHANG Jihua Shanghai Institute of Metallurgy; Academia Sinica
Cite this article: 

CHEN Shuchuan;XU Zuyao T. Y. Hsu; YANG Fan Shanghai Jiaotong University; ZHANG Jihua Shanghai Institute of Metallurgy; Academia Sinica. STABILIZATION OF MARTENSITE AND PARENT PHASE ORDERING IN A Cu-Zn-Al ALLOY. Acta Metall Sin, 1991, 27(4): 5-10.

Download:  PDF(515KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The reverse transformation has never occurred in a quenched and agedspecimen heating from room temperature to 320℃ at which the martensite disap-pears thoroughly. Both B2?9R and DO_3?18R coexist in step-quenched and short-timeisothermally treated specimen. As prolonging the isothermally holding, the B2?9Rdisappears and DO_3?18R intensifies. B2?9R occurs only in specimen quenched andup-quenched immediately to 100--150℃. Rapid quenching from high temperaturewill depress the B2→DO_3 ordering but not the A2→B2 one. A more enough concen-tration of vacancy is a necessary condition of occurrence of B2→DO_3 ordering. Thepossible mechanism for stabilization of martensite in Cu-Zn-Al alloy was alsodiscussed.
Key words:  stabilization of marteusite      A2→B2 ordering      vacancy concentration     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/5

1 Rapacioli R, Ahlers M. Scr Metall, 1977; 11: 1147
2 Delaey L, Deruyttere A, Aernoudt E, Roos J. Report 78-1978, Dept. Metalunde, Katholicke Universiteit, Leuven, Belgium, 1978
3 Dunne D P, Kennon N F. Scr Metall, 1982; 16: 729
4 祝向永,唐远永,曹明盛.中南矿冶学院学报,1981;(3) :1
5 Arab A, Ahlers M. J Phys (Paris), Colloq, 1982; 43(C4) : 709
6 Van Humbeeck J, Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984: 18: 893
7 Scarsbrook G, Cook J M, Stobbs W M. Metall Trans, 1984; 15A: 1977
8 Yan Humbeeck J, Segers D, Delaey L. Scr Metall, 1985; 19: 477
9 1969; 27: 141
No related articles found!
No Suggested Reading articles found!