INTERGRANULAR AND EXFOLIATION CORROSION BEHAVIOUR OF 8090Al-Li ALLOY
ZHANG Yun;LIU Yulin;ZHAO Hong'en;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang; ZHU Ziyong; WANG Zhengfu Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang
Cite this article: 

ZHANG Yun;LIU Yulin;ZHAO Hong'en;HU Zhuangqi Institute of Metal Research; Academia Sinica; Shenyang; ZHU Ziyong; WANG Zhengfu Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. INTERGRANULAR AND EXFOLIATION CORROSION BEHAVIOUR OF 8090Al-Li ALLOY. Acta Metall Sin, 1991, 27(4): 127-133.

Download:  PDF(2888KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Al-2.79Li-1.3Cu-0.7Mg-0.12Zr(8090 Al-Li) alloy has excellent re-sistance to intergranular and exfoliation corrosion as naturally aged, worst as peakaged and rather better as underaged than as overaged. The corrosion behaviour ofthe alloy is closely dependent on its microstructure. Under the peak aging condition,the coarse T_2 phase, which is continuously distributed along grain boundary, has solow corrosion potential in comparison with matrix, that makes the corrosion resis-tance of the alloy to be deteriorated by anodic dissolution along grain boundary.
Key words:  Al-Li alloy      pit corrosion      intergranular corrosion resistance      exfoliation behaviour     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/127

1 Reboul M, Meyer P. J Phys (Paris), Colloq, 1987; 48(C3) : 881
2 Bavarian B, Becker J, Parikh S N, Zamanzadeh M. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Vol. Ⅲ, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27-31, 1989, Birmingham (UK): Materials and Component Engineering Publications Ltd., 1989: 1227
3 Colvin E L, Murtha S J. In: Sanders T H Jr., Starke E A Jr., eds., Aluminum-Lithium Alloys, Vol. Ⅲ, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham (UK): Materials and Component Engineering Publications Ltd., 1989: 1251
4 Baumert B A, Ricker R E. In:Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium Lithium Alloys Ⅲ, Proc 3rd Int Aluminium-Lithium Conf, University of Oxford, 8--11, July, 1985, London: The Institute of Metals, 1986: 282
5 Srivatsan T S, Bobeck G E, Sudarshan T S, Molian P A. In: Sanders T H Jr., Starke E A Jr., eds., Aluminum Lithium Alloys, Vol. Ⅲ, Proc 5th Int Aluminum-Lithum Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham (UK): Materials and Component Engineering Publications Ltd.. 1989: 1237
6 韩玉梅.中国科学院金属腐蚀与防护研究所硕士研究生论文,1990@
[1] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[2] LI Shiju, LI Yang, CHEN Jianqiang, LI Zhonghao, XU Guangming, LI Yong, WANG Zhaodong, WANG Guodong. Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field[J]. 金属学报, 2020, 56(6): 831-839.
[3] Chao CAI,Yang LI,Jinfeng LI,Zhao ZHANG,Jianqing ZHANG. Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. 金属学报, 2019, 55(8): 958-966.
[4] Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG. Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy[J]. 金属学报, 2019, 55(6): 709-719.
[5] Jinfeng LI,Danyang LIU,Ziqiao ZHENG,Yonglai CHEN,Xuhu ZHANG. EFFECT OF Er MICRO-ALLOYING ON MECHANICAL PROPERTIES AND MICROSTRUCTURES OF 2055 Al-Li ALLOY[J]. 金属学报, 2016, 52(7): 821-830.
[6] Xianfeng ZHANG,Guoai LI,Zheng LU,Juan YU,Min HAO. EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. 金属学报, 2016, 52(12): 1497-1502.
[7] LIU Fenjun, FU Li, ZHANG Wenyuan, MENG Qiang, DONG Chunlin, LUAN Guohong. INTERFACE STRUCTURE AND MECHANICAL PRO-PERTIES OF FRICTION STIR WELDING JOINT OF 2099-T83/2060-T8 DISSIMILAR Al-Li ALLOYS[J]. 金属学报, 2015, 51(3): 281-288.
[8] WANG Dong DONG Chunlin XIAO Bolv GAO Cong HE Miao LUAN Guohong MA Zongyi. EFFECT OF WELDING PARAMETERS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR WELDED AlCuLi ALLOY JOINTS[J]. 金属学报, 2012, 48(9): 1109-1115.
[9] SU Jingxin; ZHANG Zhao; CAO Fahe; ZHANG Jianqing; CAO Chunan. EXFOLIATION CORROSION BEHAVIOR OF T6 TREATED 2090 Al-Li ALLOY IN EXCO SOLUTION AND EIS DURING EXFOLIATION CORROSION EVOLUTION[J]. 金属学报, 2005, 41(9): 974-978 .
[10] WU Ximao;Al Suhua;ZHANG Yun;WANG Zhonmang;HAN Xinglin (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) (Shenyang Polytechnic University. Shenyang 110023). THE LOW CYCLE FATIGUE BEHAVIOUR FOR 8090 Al-Li ALLOYS[J]. 金属学报, 1997, 33(7): 702-708.
[11] Tian Baohui (Beijing Institute of Aeronautical Materials; Beijing 100095); Li HuanxiZhang Yonggang;Chen Changqi(Beijing University of Aeronautics and Astronautics;Beijing 100083). INFLUENCING FACTORS OF SERRATED FLOW IN Al-Li SINGLE CRYSTALS[J]. 金属学报, 1997, 33(6): 577-582.
[12] LIN Zhaoqi;ZHAO Gang; LI Hongxiao; RU Hongqiang; LIU Chunming (Northeastern University; Shenyang 110006). EFFECT OF HYDROGEN CONTENT ON STRUCTURE AND PROPERTIES IN 2091-T6 Al-Li ALLOY SHEET[J]. 金属学报, 1997, 33(10): 1047-1052.
[13] PENG Delin; MIN Guanghui; AN Geying; LIU Hongbo (Harbin Institute of Technology; Harbin 150001). DIRECTIONAL GROWTH OF EUTECTIC Al-Li COMPOSITE MATERIALS[J]. 金属学报, 1996, 32(9): 993-997.
[14] HAO Chuanyong; YU Erjing; YING Huiyun; SHI Chenggen (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). NUCLEATION MECHANISM OF 8090 Al-Li ALLOY WELD METAL[J]. 金属学报, 1996, 32(6): 647-652.
[15] ZHANG Wanming; ZHANG Yun; HU Zhuangqi; LIU Yulin; ZHAO Hong'en;(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-09-15). EFFECTS OF EQUILIBRIUM PHASES ON MECHANICAL PROPERTIES OF 8090 Al-Li ALLOY[J]. 金属学报, 1996, 32(5): 484-488.
No Suggested Reading articles found!